IEICO-4Cl, low bandgap NFA with absorption into the near-infrared

Available for priority dispatch with free shipping on qualifying orders


Specifications | Pricing and Options | MSDS | Literature and Reviews


IEICO-4Cl (CAS number 2240998-88-1), a chlorinated version of IEICO-4F, has a structure with an electron-donating fused indaceno[1,2-b:5,6-b′]dithiophene (IDT) core flanked by two electron-withdrawing terminals, 2-(5,6-dichloro-3-oxo-2,3-dihydro-1H-inden-1-ylidene)malononitrile (IC-2Cl). IEICO-4Cl has an ultralow bandgap of 1.23 eV with weak absorption in the visible region, but extends its main absorption into the near-infrared (NIR) region (745-945 nm) with maximum absorption around 880 nm and an absorption onset of ≈1010 nm.

Organic tandem solar cell with PBDB-TF:IT-4F as active layer for the front cell and PTB7-Th:IEICO-4Cl:PC71BM as active layer for the real cell gained a power conversion efficiency (PCE) of 15.26%.

High efficient non-flullerene acceptor

High efficient non-fullerene acceptor

with highly conjugated core

Expanded absorption range to near infrared

Expanded absorption range to near infrared

Large dipole moment induced by chloride substituents

Worldwide shipping for 2240998-88-1

Worldwide shipping

Quick and reliable shipping

High purity

High purity

>99% High purity

Device structure: ITO/TIPD/PBDB-TF:IT-4F/m-PEDOT/TIPD/PTB7-Th:IEICO-4Cl:PC71BM/MoO3/Ag

Thickness (nm) VOC (V) JSC (mA cm-2) FF (%) PCE (%)
105/150 nm 1.58 14.36 67.27 15.26

Our high purity (>99%) IEICO-4Cl is available for priority dispatch (lead times may apply for large quantities) and ships free with qualifying orders.

General Information


CAS Number 2240998-88-1
Chemical Formula C114H114Cl4N4O4S4
Purity >99% (1HNMR)
Full Name 2,2′-((2Z,2′Z)-(((4,4,9-tris(4-hexylphenyl)-9-(4-pentylphenyl)-4,9-dihydro-s-indaceno[1,2-b:5,6-b dithiophene-2,7-diyl)bis(4-((2-ethylhexyl)oxy)thiophene 5,2-diyl))bis(methanylylidene))bis(5,6-dichloro-3-oxo-2,3-dihydro-1H-indene-2,1-diylidene))dimalononitrile
Molecular Weight 1874.22 g/mol
Absorption λmax 802 nm (in chloroform), 887 nm (in film), NIR absorption
HOMO / LUMO HOMO = -5.56 eV, LUMO = -4.23 eV; Eg = 1.33 eV [1]
Solubility Chloroform, chlorobenzene
Form Dark blue powder/crystals
Synonyms IEICO-Cl
Classification / Family NFAs, n-type non-fullerene electron acceptors, organic semiconducting materials, low band-gap small molecule, small molecular acceptor, organic photovoltaics, organic photodetectors (OPDs), polymer solar cells, NF-PSCs

Chemical Structure


Chemical structure of IEICO-4Cl
Chemical structure of IEICO-4Cl, CAS number: 2240998-88-1

Pricing


Batch Quantity Price
M2341A1 100 mg £290

MSDS Documentation

IEICO-4Cl MSDSIEICO-4Cl MSDS Sheet

Literature and Reviews


  1. Efficient Semitransparent Organic Solar Cells with Tunable Color enabled by an Ultralow-Bandgap Nonfullerene Acceptor, Y. Cui et al., Adv. Mater., 29 (43), 1703080 (2017); DOI: 10.1002/adma.201703080.
  2. Efficient Organic Tandem Solar Cells Enabled by Solution-Processed Interconnection Layer and Fine-Tuned Active Layer, R. Zeng et al., Adv. Optical Mater., 9 (21), 2101246 (2021); DOI: 10.1002/adom.202101246.
  3. Nonfullerene Acceptors for Semitransparent Organic Solar Cells, S. Dai et al., Adv. Energy Mater., 1800002 (2018); DOI: 10.1002/aenm.20180000.

Related Products


Non-Fullerene Acceptors Collection

Non-Fullerene Acceptors

Non-Fullerene Acceptors

Non-fullerene acceptors (NFAs) are a promising alternative to fullerene-based electron acceptors.

Semiconducting Polymers Collection

Semiconducting Polymers

Semiconducting Polymers

Semiconducting polymers for bulk heterojunction, OPV, OLED, OFET and perovskite interfaces and solar cell research.

Organic Conductors Collection

Organic Conductors

Organic Conductors

Organic conductors are an environmentally friendly alternative to traditional inorganic conductors.

Return to the top