It looks like you are using an unsupported browser. You can still place orders by emailing us on info@ossila.com, but you may experience issues browsing our website. Please consider upgrading to a modern browser for better security and an improved browsing experience.


Product Code M2191A1-100mg
Price $257

Tris-PCz, HTL material in TADF-OLED devices

High-purity and available online for priority dispatch, CAS No. 1141757-83-6, Sublimed ≥99.0%


Tris-PCz has a tri-carbazole back-boned structure joined at the 3 and 6 positions. The highly-conjugated carbazoles makes Tris-PCz electron-rich, which is widely used as a hole-transport layer material in TADF-OLED devices.

Due to its electron-rich nature, Tris-PCz can form exciplexes with electron-deficient materials (such as B4PyPPM) in highly-efficient OLED devices with TADF characteristics.

Tris-PCz has a high triplet energy (ET = 2.7 eV), so it is also frequently used as an exciton block layer material to effectively prevent the excitons' energy from being transferred (to the donor or acceptor) to achieve high fluorescence quantum efficiency.

General Information


CAS number 1141757-83-6
Full name 9-Phenyl-3,6-bis(9-phenyl-9Hcarbazol-3-yl)-9H-carbazole
Chemical formula C54H35N3
Molecular weight 725.28 g/mol
Absorption λmax 305 nm in DCM
Fluorescence λmax 415 nm in DCM
HOMO/LUMO HOMO = 5.6 eV, LUMO = 2.1 eV; T1 = 2.7 eV [1]
Synonyms 9,9',9''-Triphenyl-9H,9'H,9''H-3,3':6',3''-tercarbazole
Classification / Family Carbazole derivative, Fluorescent host materials, Phosphorescent host materials, Hole-transport layer materials, Exciton-blocking layer materials, TADF-OLED materials, Organic electronics, Sublimed materials.

Product Details


Purity Sublimed > 99% (HPLC)
Melting point TGA: >270 °C (0.5% weight loss)
Appearance White crystals/powder

Chemical Structure


tris-pcz, 1141757-83-6-
Chemical structure of Tris-PCz, CAS 1141757-83-6

Device Structure(s)


Device structure ITO/HATCN (10 nm)/Tris-PCz (35 nm)/10 wt.% 4CzPN:mCBP (G-EML) (3 nm)/6 wt.% 4CzPN:2 wt.% 4CzTPN-Ph:mCBP (R-EML) (2 nm)/10 wt.% 3CzTRZ:PPT (B-EML) (10 nm)/PPT (50 nm)/LiF (0.8 nm)/Al (100 nm) [2]
Colour White white light emitting device
Max. Power Efficiency 30.3 lm W−1
Max. Current Efficiency 38.6 cd/A
Max. EQE 17.6%
Device structure ITO/HATCN (10 nm)/Tris-PCz (35 nm)/10 wt.% 4CzPN:mCBP (G-EML) (5 nm)/6 wt.% 4CzPN:2 wt.% 4CzTPN-Ph:mCBP (R-EML) (4 nm)/10 wt.% 3CzTRZ:PPT (B-EML) (6 nm)/PPT (50 nm)/LiF (0.8 nm)/Al (100 nm) [2]
Colour White white light emitting device
Max. Power Efficiency 34.1 lm W−1
Max. Current Efficiency 45.6 cd/A
Max. EQE 17.0%
Device structure ITO/MoO3 (1 nm)/TAPC (20 nm)/Tris-PCz (10 nm)/Tris-PCz:B4PyPPM:3 wt% Ir(MDQ)2acac (30 nm)/B4PyPPM (50 nm)/LiF (1 nm)/Al (100 nm) [3]
Colour Red red light emitting device
Max. Power Efficiency 37.3 lm W−1
Max. Current Efficiency 33.7 cd/A
Max. EQE 20.3%
Device structure ITO (100 nm)/HATCN (10 nm)/Tris-PCz (30 nm)/mCBP (5 nm)/20 wt% of 3Ph2CzCzBN:mCBP (30 nm)/SF3-TRZ (10 nm)/ 30 wt% of Liq:SF3-TRZ (50 nm)/Liq (2 nm)/ Al (100 nm) [4]
Colour Blue blue light emitting device
Max. Power Efficiency 34.5 lm W−1
Max. Current Efficiency 41.7 cd/A
Max. EQE 17.9%
Device structure ITO/TAPC (35 nm)/Tris-PCz (10 nm)/Tris-PCz:PIM-TRZ*(1:2) (30 nm)/PIM-TRZ (60 nm)/LiF (1 nm)/Al (100 nm) [5]
Colour Green green light emitting device
Max. Power Efficiency 71.0 lm W−1
Max. Current Efficiency 52.0 cd/A
Max. EQE 18.6%
Device structure ITO/4% ReO3:Tris-PCz (60 nm)/Tris-PCz (15 nm)/Tris-PCz:CN-T2T(1:1) (25 nm)/CN-T2T (50 nm)/Liq (0.5 nm)/Al (100 nm) [6]
Colour Green green light emitting device
Max. Power Efficiency 46.5 lm W−1
Max. Current Efficiency 37.0 cd/A
Max. EQE 11.9%
Max. Luminance 73, 800 cd/m2

*For chemical structure information, please refer to the cited references

Pricing


Grade Order Code Quantity Price
Sublimed (>99% purity) M2191A1 100 mg £190
Sublimed (>99% purity) M2191A1 250 mg £380
Sublimed (>99% purity) M2191A1 500 mg £660
Sublimed (>99% purity) M2191A1 1 g £1100

MSDS Documentation


Tris-PCz MSDSTris-PCz MSDS sheet

Literature and Reviews


  1. Promising operational stability of high-efficiency organic light-emitting diodes based on thermally activated delayed fluorescence, H. Nakanotani1 et al., Sci. Rep., 3, 2127 (2013); DOI: 10.1038/srep02127.
  2. High-efficiency white organic light-emitting diodes using thermally activated delayed fluorescence, J. Nishide et al., Appl. Phys. Lett. 104, 233304 (2014); doi: 10.1063/1.4882456.
  3. High-performance red organic light-emitting devices based on an exciplex system with thermally activated delayed fluorescence characteristic, S. Yuan et al., Org. Electronics, 39, 10-15 (2016); doi: 10.1016/j.orgel.2016.09.020.

Return to the top