PNF222, polymer acceptor for all-PSCs and OFETs

High quality polymer available with free shipping on qualifying orders


Specifications | MSDS | Literature and Reviews


PNF222, poly[[1,2,3,6,7,8-hexahydro-2,7-bis(2-octyldodecyl)-1,3,6,8-tetraoxobenzophenanthroline-4,9-diyl](3,3'-difluoro[2,2'-bithiophene]-5,5'-diyl)], CAS number 1773524-46-1, is commonly used as polymer acceptor in all polymer solar cells or OFETs material.

Compared to PNDI(2OD)2T, with the introduction of the fluorine atoms on the electronic structure of the polymer, PNF222 has lower electronic energy levels due to the strong electronegativity of its fluorine atoms. In turn, this results in higher Voc, Jsc and FF for OPV devices.

It has also been reported that PCE of Si-PEDOT:PSS solar cells was promoted from 12.6% to 14.5% while a PNF222 polymer interlayer was incorporated, with the polymer orientation playing a critical role on the polymer–Si contact quality [3].

Luminosyn™ PNF222


Luminosyn™ PNF222 is now available.

High molecular weight and high purity

PNF222 is purified by soxhlet extraction with methanol, hexane and chlorobenzene under argon atmosphere

Batch-specific GPC data

Have confidence in what you are ordering; batch-specific GPC data for your thesis or publications

Large quantity orders

Plan your experiments with confidence with polymers from the same batch

General Information


CAS Number 1773524-46-1
Chemical Formula (C62H86F2N2O4S2)n
Full Name Poly[[1,2,3,6,7,8-hexahydro-2,7-bis(2-octyldodecyl)-1,3,6,8-tetraoxobenzo[lmn][3,8]phenanthroline-4,9-diyl](3,3'-difluoro[2,2'-bithiophene]-5,5'-diyl)]
Molecular Weight See Batch Details table above
HOMO / LUMO HOMO = - 5.99 eV, LUMO = - 3.90 eV [1]
Suggesting Solvents Dichlorobenzene
Synonyms PNDI-2F, P(NDI2OD-T2F), PNDI(2OD)2T-2F, P(NDI2OD-FT2)
Soluble in Chloroform, chlorobenzene, dichlorobenzene
Recommended Processing Solvents at 10mg/ml Chloroform - M2052A3, Dichlorobenzene or Chlorobenzene+dichlorobenzene (1:1 v/v)  - M2052A2
Classification / Family PNDI polymers, Bithiophene, Heterocyclic five-membered ring, Organic semiconducting materials, Low band gap polymers, Non-fullerene acceptors (NFAs), Organic photovoltaics, All-polymer solar cells, OFETs

Batch Details


Batch number MW Mn PDI Stock info
M2052A2 163,267 81,850 1.99 Low Stock
M2052A3 51,139 31,734 1.61 In Stock

Chemical Structure


PNF222 chemical structure
Chemical structure and product image of PNF222

MSDS Documentation


PNF222 MSDSPNF222 MSDS Sheet

Literature and Reviews


  1. Controlling Energy Levels and Blend Morphology for All-Polymer Solar Cells via Fluorination of a Naphthalene Diimide-Based Copolymer Acceptor, M. A. Uddin et al., Macromolecules, 49 (17), 6374–6383 (2016); DOI: 10.1021/acs.macromol.6b01414.
  2. Fluoro-Substituted n-Type Conjugated Polymers for Additive-Free All-Polymer Bulk Heterojunction Solar Cells with High Power Conversion Efficiency of 6.71%, J. Jung et al., Adv. Mater., 27, 3310–3317 (2015); DOI: 10.1002/adma.20150121.
  3. Naphthalene Diimide-Based n-Type Polymers: Efficient Rear Interlayers for High-Performance Silicon–Organic Heterojunction Solar Cells, Y. Han et al., ACS Nano, 11 (7), 7215–7222 (2017); DOI: 10.1021/acsnano.7b03090.

Return to the top