Product Code M2081A2-100mg
Price $540

PNDI(2HD)T, polymer acceptor for high performance all-PSCs

High quality polymer available for fast, secure dispatch


Specifications | MSDS | Literature and Reviews


PNDI(2HD)T, CAS number 1675973-74-6, also known as P(NDI2HD-T), is a copolymer used as a polymer acceptor in high-performance all-polymer solar cells (All-PSCs).

All-PSCs based on PBDTTTPD and PNDI(2HD)T exhibited a PCE of 6.64% with better flexibility, stretching, and bending properties when compared to polymer solar cells with PCBMs as acceptors. The high performances of these devices with P(NDI2HD-T) as polymer acceptor was due to the high open circuit voltage (1.06 V) and favourable interfacial interactions between the active layers of polymer donor and acceptor.

It has also been demonstrated that a combination of polymer and small molecule acceptors, such as P(NDI2HD-T)/ITIC with only a small amount of ITIC in presence, significantly improves the device PCE from 6% to over 7% when PTP8 was used as polymer donor [5].

Luminosyn™ PNDI(2HD)T


Luminosyn™ PNDI(2HD)T (also referred to as P(NDI2HD-T)) is now available.

Higher molecular weights and high purity

PNDI(2HD)T is purified via Soxhlet extraction with methanol, hexane and chlorobenzene under an argon atmosphere

Batch-specific GPC data

Have confidence in what you are ordering; batch-specific GPC data for your thesis or publications

Large quantity orders

Plan your experiments with confidence with polymers from the same batch

General Information


Full name Poly{[N,N'-bis(2-hexylldecyl)naphthalene-1,4,5,8-bis(dicarboximide)-2,6-diyl]-alt-2,5-thiophene}
Synonyms
  • P(NDI2HD-T)
  • PNDI-T-HD
  • Polynaphthalene diimide-thiophene
Chemical formula (C50H70N2O4S)n
CAS number 1675973-74-6
HOMO / LUMO HOMO = -5.64 eV, LUMO = -3.79 eV [1]
Classification / Family PNDI polymers, Organic n-type semiconducting materials, Organic photovoltaics, All-polymer solar cells (All-PSCs), Electron-acceptor polymers, OPV acceptors, OFETs, Perovskite solar cells.
Soluble in Chloroform, chlorobenzene, dichlorobenzene
Recommended Processing Solvents at 10mg/ml Chloroform, chlorobenzene

Batch Details


Batch number MW Mn PDI Stock info
M2081A1 267,653 148,132 1.81 Discontinued
M2081A2 193,704 105,414 1.84 In stock

Chemical Structure


P(NDI2HD-T)
Chemical structure and product image of P(NDI2HD-T)

MSDS Documentation


PNDI(2HD)T MSDSPNDI(2HD)T MSDS Sheet

Literature and Reviews


  1. Flexible, highly efficient all-polymer solar cells, T. Kim et al., Nat. Commun., 6, 8547 (2015); DOI: 10.1038/ncomms9547.
  2. Impact of highly crystalline, isoindigo-based small molecular additives for enhancing the performance of all-polymer solar cells, H-H. Cho et al., J. Mater. Chem. A, 5, 21291–21299 (2017); DOI: 10.1039/c7ta06939a.
  3. Comparative Study of Thermal Stability, Morphology, and Performance of All-Polymer, Fullerene–Polymer, and Ternary Blend Solar Cells Based on the Same Polymer Donor, T. Kim et al., Macromolecules, 50 (17), 6861–6871 (2017);
    DOI: 10.1021/acs.macromol.7b00834.

Return to the top