Product Code M2051A2-100mg
Price $567

PDPP4T-2F, semiconducting polymer with deep HOMO level

High quality polymer available for fast, secure dispatch


Specifications | MSDS | Literature and Reviews


PDPP4T-2F is the fluorinated version of PDPP4T with a device performance PCE of 7.59% [1].

In comparison to PDPP4T, PDPP4T-2F has a deeper highest-occupied molecular orbital (HOMO) level, due to the electron-withdrawing nature of the fluorine atoms on the thiophene units. It has also been reported that apart from being more favorable for realising higher Voc due to its deeper HOMO energy level, PDPP4T-2F shows great potential in achieving a higher Jsc than PDPP4T in devices for its improved extinction coefficient.

General Information


Full name Poly[2,5-bis(2-octyldodecyl)pyrrolo[3,4-c]pyrrole-1,4(2H,5H)-dione -3,6-diyl)-alt-(3'',​4'-​difluoro[2,2’;5’,2’’;5’’,2’’’-quaterthiophen]-5,5’’’-diyl)]
Synonyms PFDPP4T, PDQT-2F
CAS number n/a
Chemical formula (C62H88F2N2O2S4)n
Molecular weight See Batch Details table
HOMO / LUMO HOMO = ~ 5.22 eV, LUMO = ~ 3.66 eV [3]
Soluble in Chloroform, chlorobenzene, dichlorobenzene
Recommended Processing Solvents at 10mg/ml Chloroform (2mg/ml)
Classification / Family Quaterthiophene, Heterocyclic five-membered ring, Organic semiconducting materials, Low band gap polymers, Organic photovoltaics, Polymer solar cells, OFETs

Batch Details


Batch Mw Mn PDI Stock Info
M2051A1 173,151 63,296 2.74 Out of stock
M2051A2 70.758 33,458 2.11 In Stock

Chemical Structure


PDPP4T-2F chemical structure
Chemical structure of PDPP4T-2F

MSDS Documentation


PDPP4T-2F MSDSPDPP4T-2F MSDS sheet

Literature and Reviews

  1. Sequential Deposition: Optimization of Solvent Swelling for High-Performance Polymer Solar Cells, Y. Liu et al., ACS Appl. Mater. Interfaces, 7, 653-661 (2015); DOI: 10.1021/am506868g.
  2. Effect of Fluorination on Molecular Orientation of Conjugated Polymers in High Performance Field-Effect Transistors, A. Zhang et al., Macromolecules, 49 (17), 6431–6438 (2016); DOI: 10.1021/acs.macromol.6b01446.
  3. Over 11% Efficiency in Tandem Polymer Solar Cells Featured by a Low-Band-Gap Polymer with Fine-Tuned Properties, Z. Zheng et al., Adv. Mater., 28, 5133–5138 (2016); DOI: 10.1002/adma.201600373.
Return to the top