It looks like you are using an unsupported browser. You can still place orders by emailing us on info@ossila.com, but you may experience issues browsing our website. Please consider upgrading to a modern browser for better security and an improved browsing experience.


Product Code M2211C1-500mg
Price $297

Low price, high purity 2D nickel phosphorus trisulfide powder and crystal

For the development of next-generation electronics, optoelectronics, and nanotechnology


Technical Data | MSDS | Structure | Literature and Reviews | Related Products | Resources and Support


Nickel phosphorus trisulfide (NiPS3) is a layered quasi-two dimensional antiferromagnetic (AFM) semiconductor (TN=155 K). Nickel phosphorus trisulfide (NiPS3) belongs to the group of 2D layered transition metal phosphorus trichalcogenides (MPX3). Among them, NiPS3 has quite unique physical properties with capability of both p-type and n-type doping for device applications and the smallest bandgap energy (~1.6 eV).

NiPS3 high purity Crystal

High Purity

NiPS3 ≥99.999% high purity crystal

Powder & Crystal Nickel Phosphorus Trisulfide

Powder & Crystal

Powder & Crystal Forms

Low Cost Nickel Phosphorus Trisulfide

Low Cost

Low Cost Nickel Phosphorus Trisulfide

Nickel Phosphorus Trisulfide Applications

Applications

Development of next-generation electronics, optoelectronics, and nanotechnology

The antiferromagnetic ordering in NiPS3 is persistent down to two-layer nano-structures and is substantially suppressed in the monolayer, unlike the case of Ising-type antiferromagnet FePS3 in which antiferromagnetic ordering maintains down to the monolayer limit. Antiferromagnetic van der Waals material NiPS3 offers a good model system for the XY Hamiltonian or XXZ-type, while FePS3 of anistropic Ising-type and MnPS3 of isotropic Heisenberg-type.

Nickel phosphorus trisulfide powder

Nickel Phosphorus Trisulfide Powder

Can be used for preparation of nickel phosphorus trisulfide nanoplates and ultrathin films

Available in quantities of 1 g

≥99.995% purity

From £350

Nickel phosphorus trisulfide by size

Nickel Phosphorus Trisulfide Crystals by Size

Can be used to produce single or few-layer nickel phosphorus trisulfide sheets via mechanical or liquid exfoliation

Small (≥10 mm2) or medium (≥25 mm2) crystals available*

≥99.999% purity

From £520

*Typical representative size, areas/dimensions may vary

Bulk single nickel phosphorus trisulfide crystal is most commonly used as sources from which single or few-layer sheets can be obtained via either mechanical or liquid exfoliation. Single nickel phosphorus trisulfide crystal or films produced from such crystals are suitable for study using atomic force microscopy or transmission electron microscopy.

Few-layer NiPS3 nanosheets and nanoparticles can also obtained from nickel phosphorus trisulfide powder by liquid-exfoliation.

Technical Data

CAS Number N/A
Chemical Formula NiPS3
Molecular Weight 185.86 g/mol
Bandgap ~1.6 eV (in bulk)
Preparation Synthetic - Chemical Vapour Transport (CVT)
Structure Monoclinic
Electronic Properties 2D Magnetic semiconductor
Melting Point N/A
Colour Green
Synonyms Nickel phosphosulphide, Nickel thiophosphate, Nickel phosphorous trisulphide
Classification / Family 2D layered transition metal phosphorus trichalcogenides (MPX3), Magnetic semiconductor, Antiferromagnet, Nano-electronics, Nano-photonics, Photovoltaic, Materials science

Product Details

Form Purity
Powder ≥99.995%
Crystal ≥99.999%

Pricing Table

Product Code Form Size/Weight* Price
M2211C1 Powder 500 mg £220
M2211C1 Powder 1 g
£350
M2211A10 Crystal Small (≥10 mm2) £520 ea.
M2211A25 Crystal Medium (≥25 mm2) £850 ea.

*typical representative size, areas/dimensions may vary.

Shipping is free for qualifying orders placed via our secure online checkout.

MSDS Documents


Nickel phosphorus trisulfide powder MSDSNickel phosphorus trisulfide powder

Nickel phosphorus trisulfide crystal MSDSNickel phosphorus trisulfide crystal

Structure of Nickel Phosphorus Trisulfide


NiPS3 crystalises in monoclinic crystal structure containing two molecular formula units per unit cell (Ni2P2S6). NiPS3 consists of layers of covalently bonded clusters of [P2Se6]4-dumbbell bipyramids with honeycomb arrangement of divalent nickel ions. Individual layers are bound via weak van der Waals and can be easily separated into few-layer nanosheets by either mechanical or liquid exfoliation.

NiPS3 - nickel phosphorus trisulfide crystal structure
The crystal structure of single-layer nickel phosphorus trisulfide (NiPS3)

Literature and Reviews


  1. Magnetic structure of the quasi-two-dimensional antiferromagnet, NiPS3, A. Wilde et al., Phys. Rev. B, 92, 224408 (2015); doi: 10.1103/PhysRevB.92.224408.
  2. Charge-Spin Correlation in van der Waals Antiferromagnet NiPS3, S. Kim et al., Phys. Rev. Lett. 120, 136402 (2018); doi: 10.1103/PhysRevLett.120.136402.
  3. The magnetic exchange parameters and anisotropy of the quasi-two dimensional antiferromagnet NiPS3, D. Lançon et al., hys. Rev. B, 98, 134414 (2018); doi: 10.1103/PhysRevB.98.134414.

We stock a wide range of 2D materials available to purchase online. Please contact us if you cannot find what you are looking for.

Resources and Support


Viscoelastic Transfer of 2D Material Using PDMS

Viscoelastic transfer using polydimethylsiloxane (PDMS) stamps is one of the methods used for the deterministic placement of 2D materials and the fabrication of van der Waals heterostructures. It relies on the viscoelasticity of PDMS, which behaves as an elastic solid on short time scales, but as a viscous fluid on long time scales.

Learn more...
Return to the top