Substrate Rack
Rack to hold 20 substrates for a variety of processing techniques. Manufactured from polypropylene to resist most solvents and acids used in organic electronics processes including THF, toluene, xylene, chloroform, chlorobenzene, dichlorobenzene and trichlorobenzene.
Further InformationMost commonly used for cleaning substrates, the racks are also useful for many other batch processes including solvent annealing, deposition of self-assembled monolayers, low-temperature baking and of course storage. The Substrate Rack (for 20x15mm substrates) is designed to fit perfectly inside our polypropylene beaker which allows annealing and cleaning of substrates with minimum solvent waste.
Specifications | E101 | E102 |
Size | 86 mm x 27 mm x 10 mm | 86 mm x 32 mm x 20 mm |
Holds | 20 substrates of 15 x 20 mm, thickness up to 1.5mm | 20 substrates of 25 x 25 mm (or 25 x 75mm), thickness up to 1.5mm |
Material | Injection Moulded Polypropylene | Die Cast Polypropylene |

Substrate Cleaning Routine
The video below demonstrates the way in which our substrate rack can be used during the process of cleaning substrates in preparation for fabricating PV/LED devices.
To the best of our knowledge the information provided here is accurate. However, Ossila assume no liability for the accuracy of this page. The values provided are typical at the time of manufacture and may vary over time and from batch to batch. All products are for laboratory and research and development use only, and may not be used for any other purpose including health care, pharmaceuticals, cosmetics, food or commercial applications.