FREE shipping to on qualifying orders when you spend or more. All prices ex. VAT.

ITO Glass Substrates, 20 x 15 mm, PV and OLED


Product Code S211
Price $260.00 ex. VAT

Pre-patterned ITO Glass substrates for OPV/OLED testing. Use with our cathode deposition mask (E501) to create 8 individual pixels or (E502) to create a single large pixel.

 

Datasheet

Substrate specifications.
Substrate size 20 mm x 15 mm
Thickness 1.1 mm
Glass type Polished soda lime, float glass
Substrate coating Fully oxidized ITO
ITO thickness 100 nm
ITO resistance 20 Ω / square
Glass roughness < 1 nm RMS (By AFM)
ITO roughness 1.8 nm RMS (By AFM)

 

ITO photovoltaic substrate (8 pixel) schematic

 

AFM scan of ITO substrate
10 µm x 10 µm AFM scan with Z-scale of ±5 nm.

 

AFM of glass surface of ITO substrates
AFM of glass surface (1 µm x 1 µm x 3.5 nm). Courtesy of Richard T Grant.

 

ITO Transmittance
Transmittance of ITO substrates

 


To the best of our knowledge the information provided here is accurate. However, Ossila assume no liability for the accuracy of this page. The values provided are typical at the time of manufacture and may vary over time and from batch to batch. All products are for laboratory and research and development use only, and may not be used for any other purpose including health care, pharmaceuticals, cosmetics, food or commercial applications.