ITO Glass Substrates, 20 x 15 mm, PV and OLED
Pre-patterned ITO Glass substrates for OPV/OLED testing. Use with our multi electrode cathode deposition mask to create 8 individual pixels or single electrode deposition mask to create a single large pixel.
Specifications
Substrate size | 20 mm x 15 mm |
Thickness | 1.1 mm |
Glass type | Polished soda lime, float glass |
Substrate coating | Fully oxidized ITO |
ITO thickness | 100 nm |
ITO resistance | 20 Ω / square |
Glass roughness | < 1 nm RMS (By AFM) |
ITO roughness | 1.8 nm RMS (By AFM) |

Characterisation


Transmittance of ITO Substrates

To the best of our knowledge the information provided here is accurate. However, Ossila assume no liability for the accuracy of this page. The values provided are typical at the time of manufacture and may vary over time and from batch to batch. All products are for laboratory and research and development use only, and may not be used for any other purpose including health care, pharmaceuticals, cosmetics, food or commercial applications.