ITO Glass Substrates, 75 x 25 mm, PV and OLED


Product Code S251
Price $160.00 ex. VAT

25 X 75 mm ITO patterned glass substrate, available with either modules or pixelated design. Perfect for use in OPV and OLED research.

The Pixelated Substrate System and Mini-Module Substrate System are designed to enable affordable scale-up. Alongside the Scale-Up Substrate Evaporation Masks, the substrates allow for larger devices and investigation of large-scale manufacturing techniques. 

Datasheet

Size 25 mm x 75 mm
Thickness 1.1 mm
Glass type Polished soda lime, float glass
Substrate coating Fully oxidised ITO
ITO thickness 100 nm
ITO resistance 20 Ω/square
Glass roughness Less than 1 nm RMS (by AFM)
ITO roughness 1.8 nm RMS (by AFM)

Dimensions

Dimensionised drawing of the Pixelated OPV/OLED Scale-up Substrate
Dimensionised drawing of the Pixelated OPV/OLED Scale-up Substrate
Dimensionised drawing of the Modules OPV/OLED Scale-up Substrate
Dimensionised drawing of the Modules OPV/OLED Scale-up Substrate

To the best of our knowledge the information provided here is accurate. However, Ossila assume no liability for the accuracy of this page. The values provided are typical at the time of manufacture and may vary over time and from batch to batch. All products are for laboratory and research and development use only, and may not be used for any other purpose including health care, pharmaceuticals, cosmetics, food or commercial applications.

Return to the top