ITO Glass Substrates, 20 x 15 mm (Legacy, Generation II)


Product Code S171
Price $264.00 ex. VAT

Pre-patterned ITO substrates for OPV/OLED testing. Use with our E345 cathode deposition mask to create six small pixels with areas 4 mm2 each or use our E346 mask to create a single large pixel of 50 mm2. Optional active area deposition masks (E355/E356) also available to enable vacuum deposition of active layers or inter-layers.

There is a newer version of this product. Our generation I and II substrates and masks will be discontinued soon and are only available while stocks last. Please contact us for further details.

Datasheet

Substrate size 20 mm x 15 mm
Thickness 1.1 mm
Pixel dimensions (with E345 small cathodes) 2 mm x 2 mm (4 mm2)
Pixel dimensions (with E346 large cathodes) 10mm x 5mm (50 mm2)
Glass type Polished soda lime, float glass
Substrate coating Fully oxidized ITO
ITO thickness 100 nm
ITO resistance 20 Ω / square
Glass roughness <1 nm rms By AFM
ITO roughness 1.8 nm RMS (By AFM)
Pixelated cathode substrate
Pixelated cathod substrate.
Pixelated cathode substrate schematic
Dimensionalised image of ITO Glass Substrate.
AFM scan of ITO substrate
10 µm x 10 µm AFM scan with Z-scale of ±5 nm.
AFM of glass surface of ITO substrates
AFM of glass surface (1 µm x 1 µm x 3.5 nm).
Transmittance of ITO
Transmittance of ITO substrates.

To the best of our knowledge the information provided here is accurate. However, Ossila assume no liability for the accuracy of this page. The values provided are typical at the time of manufacture and may vary over time and from batch to batch. All products are for laboratory and research and development use only, and may not be used for any other purpose including health care, pharmaceuticals, cosmetics, food or commercial applications.