ITO Glass Substrates, 75 x 25 mm, OFET and Sensing
A 25 X 75 mm version of our popular Interdigitated ITO Substrates for OFET and Sensing.
The Scale-Up and Mini-Module Substrate System is designed to enable affordable scale up. Alongside the Scale Up Substrate Evaporation Masks, the substrates allow for larger devices and investigation of large scale manufacture techniques.
Datasheet
Size | 25 mm x 75 mm |
Thickness | 1.1 mm |
Glass type | Polished soda lime, float glass |
Substrate coating | Fully oxidized ITO |
ITO thickness | 100 nm |
ITO resistance | 20 Ω/square |
Glass roughness | Less than 1 nm RMS (by AFM) |
ITO roughness | 1.8 nm RMS (by AFM) |
Dimensions