Lithium manganese oxide (LMO), CAS number 12057-17-9, has a chemical formula of LiMn2O4. It is a promising candidate to replace layered Ni or Co oxide materials as the cathode in lithium-ion batteries for its intrinsic low-cost, environmental friendliness, high abundance, and better safety. Lithium manganese oxide can improve ion transport and power capability especially at high rates with higher nominal voltage (4.0 V) than the benchmark cathode material LiCoO2.

improved ion transport 12057-17-9

High voltage

Improve ion transport at higher rates with High Voltage

Environmentally friendly Lithium Manganese Oxide (LMO) Powder

Environmentally friendly

Improved environmental friendliness

Low Cost Lithium Nickel Manganese Oxide

Low Cost

Intrinsic low-cost

safe 12057-17-9

Safety

Better safety

Lithium manganese oxide has a spinel crystal structure with space group of Fd3m. Closely packed oxygen array allocates cations in octahedral and tetrahedral sites. The same amount of Mn3+ and Mn4+ occupies the octahedral sites while lithium occupies the tetrahedral sites.

lithium manganese oxide crystal structure
Lithium manganese oxide (LiMn2O4) crystal structure, CAS 12057-17-9

Like LiCoO2, LiMn2O4 also suffers from capacity fading caused by a combination of structural transformation and transition metal cation dissolution. The so called Jahn–Teller distortion, occurred at the discharge state of Mn3+, causes a symmetry distortion of the octahedra complex and transforms the spinel into a tetragonal with large anisotropic volume change. The structure distortion is peaked at high current rate when Li+ diffusion rate into the electrolyte is greater than inside the domain of the crystal structure.

Technical Data


CAS Number 12057-17-9
Chemical Formula LiMn2O4
Molecular Weight 180.81 g/mol
Chemical Name Lithium Manganese Oxide
Synonyms Lithium manganese oxide spinel powder
Classification / Family 2D semiconducting materials, Battery materials, Metal oxides, Cathode materials
Colour Black to grey powder
Melting Point 400 °C

Product Detail


Product Code M2402A1 M2402A2
Average Particle Size (APS) D50: 23 – 27 μm D50: 14.8 μm
Specific Surface Area (SSA) 0.4 – 1.0 m2/g 0.68 m2/g
Coin Cell Capacity 0.1 C ~105 mAh/g 115.9 mAh/g

*For larger orders please email us to discuss prices.

MSDS Documents


Lithium Manganese Oxide (LiMn2O4) Powder MSDSLithium Manganese Oxide (LMO) Powder MSDS Sheet

Literatures


  1. High Performance LiMn2O4 Cathode Materials Grown with Epitaxial Layered Nanostructure for Li-Ion Batteries, M. Lee et al., Nano Lett., 14 (2), 993–999 (2014); DOI: 10.1021/nl404430e.
  2. High-rate cyclability and stability of LiMn2O4 cathode materials for lithium-ion batteries from low-cost natural β−MnO2, J. Abou-Rjeily et al., Energy Stor. Mater., 26, 423-432 (2020); DOI: 10.1016/j.ensm.2019.11.015.
  3. Core-shell structure of LiMn2O4 cathode material reduces phase transition and Mn dissolution in Li-ion batteries, C. Tomon et al., Commun. Chem., 5, 54 (2022): DOI: 10.1038/s42004-022-00670-y.

We stock a wide range of Battery Materials available to purchase online. Please contact us if you cannot find what you are looking for.

Cathode Active Materials Collection

Cathode Active Materials

Cathode Active Materials

Explore the range of high-purity cathode materials including NMC and LCO

Metal Oxide Collection

Metal Oxides

Metal Oxides

A range of metal oxides for application in batteries and much more.

Anode Active Materials Collection

Anode Active Materials

Anode Active Materials

Explore the range of anode active materials including graphite.

Return to the top