Lithium Iron Phosphate (LiFePO4) Powder
CAS Number 15365-14-7
2D Materials, Battery Materials, Cathode Active Materials, Green Energy Materials, Inorganic Electronic Materials, Low Dimensional Materials,Lithium Iron Phosphate (LiFePO4) Powder, LFP Cathode Material
Desirable high specific energy capacity LFP cathode material for mass production in electrical vehicles
Technical Data | Crystal Structure | MSDS | Literature and Reviews | Related Products
Lithium iron phosphate (LiFePO4 - CAS number 15365-14-7) also known as lithium ferro phosphate (LFP), for use as the cathode material for LFP batteries. LiFePO4 has high specific energy (90 – 170 Wh Kg-1), high volumetric energy density (1200 kJ L-1) and offer good cyclic performance (~1500 cycles) with nominal cell voltage (~3.2 Vs. Li/Li+).
Lithium iron phosphate has a wide but flat exothermic reaction peak at 250 – 360 °C with a much smaller heat release of 147 J g-1. The strong P–O covalent bond prohibits oxygen release thus promoting intrinsic safety which is the top priority of an electrical vehicles (EVs). Also with relatively Low cost, long battery life, no cobalt content, it makes LFP battery cells desirable for mass production for in EVs.
Long Battery Life
Desirable for mass production
Low Cost
Cost Effective Value
High Safety
Prohibiting oxygen release
Worldwide Shipping
Quick and reliable shipping
Lithium iron phosphate (LFP) powder consists of various chemical components that contribute to its excellent cathode performance. Its crystal structure is highly stable, thanks to a robust phosphate framework that resists distortion. Iron serves as the redox center and remains within the structure during cycling, helping maintain structural integrity despite ongoing redox activity.
Technical Data
CAS Number | 15365-14-7 |
---|---|
Chemical Formula | LiFePO4 |
Molecular Weight | 157.76 g/mol |
Chemical Name | Lithium Iron Phosphate |
Synonyms | Lithium Ferro Phosphate, LFP, LFPO |
Classification / Family | 2D semiconducting materials, Battery materials, Metal oxides, Cathode materials |
Colour | Black powder |
Lithium Iron Phosphate (LiFePO4) Powder
Product Code | M2408A1 |
---|---|
Resistance | 115 Ω cm |
Tap Density | 1.13 g/cm3 |
SSA | 12.2 m2/g |
Particle Size | ~1.5 µm (D50) |
pH | ≤8.9 |
Discharge Efficiency (First) | 97.5% |
Capacity (First) | 155.5 mAh/g |
Crystal Structure
The triphylite lithium iron phosphate (LiFePO4) belongs to the olivine family of lithium ortho-phosphates. LiFePO4 has an orthorhombic crystal lattice structure in the space group Pnma. The unit cell structure is represented by corner-shared FeO6 octahedra and edge-shared LiO6 octahedra running parallel to the b-axis, linked together by the PO4 tetrahedra.

When lithium iron phosphate is coated with 2 wt% of the electrochemically exfoliated graphene layers, it is able to reach 208 mAh g-1 in specific capacity. Binder-free SWCNT modified LFPO cathode delivers a superior rate capacity of 161.5 mAh g-1 at 0.5 C and 130.2 mAh g-1 at 5 C, with a high-rate capacity retention of 87.4% after 200 cycles at 2 C.
MSDS Documents
Lithium Iron Phosphate (LiFePO4) Powder MSDS Sheet
Pricing Table
Product Code | Weight | Price |
---|---|---|
M2408A1 | 100 g | £160 |
M2408A1 | 250 g | £320 |
M2408A1 | 500 g | £512 |
*For larger orders please email us to discuss prices
Literatures
-
Thermally modulated lithium iron phosphate batteries for mass-market electric vehicles, X. Yang et al., Nat. Energy, 6, 176–185 (2021); DOI: 10.1038/s41560-020-00757-7.
-
Graphene-modified LiFePO4 cathode for lithium ion battery beyond theoretical capacity, L. Hu et al., Nat. Commun., 4, 1687 (2013): DOI: 10.1038/ncomms2705.
-
Recent Development in Carbon-LiFePO4 Cathodes for Lithium-Ion Batteries: A Mini Review, B. Ramasubramanian et al., Batteries, 8(10), 133 (2022); DOI: 10.3390/batteries8100133.
Related Products
We stock a wide range of Battery Materials available to purchase online. Please contact us if you cannot find what you are looking for.