Ir(MDQ)2(acac), phosphorescent emitter employed in OLEDs
Bright and efficient orange-red light emitter
Ir(MDQ)2(acac) has a 2-methyldibenzo[f,h]quinoxaline ligand that coordinates with the iridium metal center via the formation of Ir-N and Ir-C bonds.
Ir(MDQ)2(acac) is another family member of iridium complexes, which are the most effective phosphorescent emitters employed in OLEDs. Devices based on Ir(MDQ)2(acac) emit orange-red light, with a maximum emission of 600-614 nm. OLEDs with Ir(MDQ)2(acac) as an emitting layer material give great brightness and exceedingly-high external quantum, current, and power efficiencies.
High performance red organic electroluminescent devices based on a trivalent iridium complex with stepwise energy levels, Y. Li et al., : RSC Adv., 6, 71282 (2016); DOI: 10.1039/c6ra16517f.
Highly Efficient White Organic Light-Emitting Diodes with Ultrathin Emissive Layers and a Spacer-Free Structure, S. Wu et al., Sci. Rep., 6:25821 (2016); DOI: 10.1038/srep25821.
New Iridium Complexes as Highly Efficient Orange–Red Emitters in Organic Light‐Emitting Diodes, J. Duan et al., Adv. Mater., 15 (3), 224-228 (2003); doi: 10.1002/adma.200390051.
Highly Simplified Reddish Orange Phosphorescent Organic Light-Emitting Diodes Incorporating a Novel Carrier- and Exciton-Confining Spiro-Exciplex-Forming Host for Reduced Efficiency Roll-off, T. Xu et al., ACS Appl. Mater. Interfaces, 9, 2701−2710 (2017); DOI: 10.1021/acsami.6b13077.
To the best of our knowledge the information provided here is accurate. However, Ossila assume no liability for the accuracy of this page. The values provided are typical at the time of manufacture and may vary over time and from batch to batch. All products are for laboratory and research and development use only, and may not be used for any other purpose including health care, pharmaceuticals, cosmetics, food or commercial applications.