Guanidinium Bromide
Guanidinium bromide (GDBr) and its derivatives are known to promote and enable stable 2D perovskite structures. This is done via i) the van der Waals interactions between guanidinium cations, and ii) hydrogen−halogen bonding between guanidinium cations and halide ions of different layers.
The presence of the guanidinium cation results in reduced defect density for the perovskite film and a longer carrier lifetime, due to a hydrogen-bonding effect produced by hydrogen from the guanidinium salt.
General Information
CAS number | 19244-98-5 |
Chemical formula | CH6BrN3 |
Molecular weight | 139.98 g/mol |
Synonyms | Guanidine hydrobromide, Guanidine monohydrobromide, GDBr |
Classification / Family | Guanidinium halides, Perovskite precursor materials, Perovskite solar cells, Perovskite LEDs |
Product Details
Purity | 98% |
Melting point | 191 °C |
Colour | White Powder/crystals |
Chemical Structure

MSDS Documentation
Guanidinium bromide MSDS sheet
Literature and Reviews
- Guanidinium: A Route to Enhanced Carrier Lifetime and Open-Circuit Voltage in Hybrid Perovskite Solar Cells, N. De Marco et al., Nano Lett., 16 (2), 1009–1016 (2016); DOI: 10.1021/acs.nanolett.5b04060.
- Guanidinium benefit, O. Graydon, Nat. Photonics 10, 145 (2016); doi:10.1038/nphoton.2016.35.
- Mixed Iodide–Bromide Methylammonium Lead Perovskite-based Diodes for Light Emission and Photovoltaics, L. Gil-Escrig et al., J. Phys. Chem. Lett., 6 (18), 3743–3748 (2015); DOI: 10.1021/acs.jpclett.5b01716.
-
Luminescent and Photoconductive Layered Lead Halide Perovskite Compounds Comprising Mixtures of Cesium and Guanidinium Cations, O. Nazarenko et al., Inorg. Chem., 56 (19), 11552–11564 (2017); DOI: 10.1021/acs.inorgchem.7b01204.
- Synthesis, Crystal Structures, Optical Properties, and Phase Transitions of the Layered Guanidinium-Based Hybrid Perovskites [C(NH2)3]2MI4; M = Sn, Pb, M. Daub et al., Eur. J. Inorg. Chem., 1120–1126 (2017); DOI: 10.1002/ejic.201601499.
To the best of our knowledge the information provided here is accurate. However, Ossila assume no liability for the accuracy of this page. The values provided are typical at the time of manufacture and may vary over time and from batch to batch. All products are for laboratory and research and development use only, and may not be used for any other purpose including health care, pharmaceuticals, cosmetics, food or commercial applications.