Deposition Masks, 75 x 25 mm


Product Code E601-SPC
Price $325.00 ex. VAT

A top-contact evaporation mask, compatible with the Ossila Scale-Up and Mini-Module substrate system.

There are two designs for pixelated OLED/ OPV: 12 pixel or 24 pixel.

Thanks to an optional spacer, the mask can be used in either direct contact with the substrate, or slightly removed from the surface. The mask comes with a lid to secure the substrates to the mask using wing nuts. 

Mask with direct contact (no spacer): For sputtering and other non-directional deposition systems, as well as for thermal deposition systems with oblique angles or a very short throw, we recommend the use of the direct contact mask to get well-defined edges.

Mask with 200 μm spacer: For normal thermal evaporation systems we recommend the use of masks with the 200 μm spacer to help avoid scratches and allow better out-gassing.

 

Design and Dimensions

12 Pixel

The 12 Pixel Mask
A Dimensionalised Image of the 12 Pixel Mask

24 Pixel

The 24 Pixel Mask
A Dimensionalised Image of 24 Pixel Mask

To the best of our knowledge the information provided here is accurate. However, Ossila assume no liability for the accuracy of this page. The values provided are typical at the time of manufacture and may vary over time and from batch to batch. All products are for laboratory and research and development use only, and may not be used for any other purpose including health care, pharmaceuticals, cosmetics, food or commercial applications.