bis-PCBM (PC60BM Bisadduct)
Bis(1-[3-(methoxycarbonyl)propyl]-1-phenyl)-[6,6]C62 or bis[C60]PCBM, a PCBM bisadduct to increase the open circuit voltage of solar cells by approximately 0.1 V due to the higher lying LUMO level [1]. Also used in crystallisation studies, especially when comparing polymer-fullerene packing [2,3].
General Information
Mw | 1101.1 g/mol |
Purity | >99.5% |
CAS number | 1048679-01-1 |
MSDS Documentation
Literature and Reviews
- Fullerene Bisadducts for Enhanced Open-Circuit Voltages and Efficiencies in Polymer Solar Cells, M. Lenes et al., Advanced Materials, 20, 2116 (2008)
- Tuning the Properties of Polymer Bulk Heterojunction Solar Cells by Adjusting Fullerene Size to Control Intercalation, N. Cates et al., Nano Letters, 9, 4153 (2009)
- Effects of Intercalation on the Hole Mobility of Amorphous Semiconducting Polymer Blends, N. Cates et al., Chemistry of Materials, 22, 3543 (2010)
To the best of our knowledge the information provided here is accurate. However, Ossila assume no liability for the accuracy of this page. The values provided are typical at the time of manufacture and may vary over time and from batch to batch. All products are for laboratory and research and development use only, and may not be used for any other purpose including health care, pharmaceuticals, cosmetics, food or commercial applications.