It looks like you are using an unsupported browser. You can still place orders by emailing us on info@ossila.com, but you may experience issues browsing our website. Please consider upgrading to a modern browser for better security and an improved browsing experience.


Product Code M2258A1-100mg
Price $540

Specifications | MSDS | Literature and Reviews


PBBTSiD (CAS number 1334032-16-4) is a small bandgap copolymer (Eg = ~ 0.7 eV ) with a backbone alternating electron donating dithienosilole (DTS) and electron accepting fused-ring benzobisthiadiazole (BBT) units.

The balanced ambipolarity of the BBT moiety of the polymer makes PBBTSiD a good candidate for logic circuit applications. Integrating BBT backboned semiconducting polymers into the bottom gate/top contact TFTs resulted in balanced ambipolar performances with the high µh and µe charge mobility values.

For 5 - 10 grams order quantity, the lead time is 4-6 weeks.

Luminosyn™ PBBTSiD


Luminosyn™ PBBTSiD is now available.

High purity
PBBTSiD is purified via Soxhlet extraction with acetone, hexane, and chlorobenzene under an argon atmosphere

Large quantity orders
Plan your experiments with polymers from the same batch

General Information


Full name Poly[(4,7-bis(3-hexylthien-2-yl)- 2λ4δ2-benzo[1,2-c;4,5-c′]bis[1,2,5] thiadiazole)-alt-(3,3'-bis(2-ethylhexylsilyene-2,2'-bithiophene)]
Synonyms PBBTSiD
Chemical formula (C50H64N4S 6Si )n
CAS number 1334032-16-4
HOMO / LUMO HOMO = -4.80 eV, LUMO = -4.10 eV; Eg = ~ 0.7 eV [1]
Soluble in Chloroform, chlorobenzene and dichlorobenzene
Recommended Processing Solvents at 10mg/ml Dichlorobenzene
Classification / Family Organic semiconducting materials, Very low-bandgap polymers, Ambipolar semiconducting polymers, OFET polymers, High charge mobility polymers, Photodetectors, Thin-film Transistors

Batch Details


Batch Mw Mn PDI Stock Info
M2258A1 17,975 7,554
2.38 In stock

Chemical Structure


pbbtsid chemical structure
Chemical structure of PBBTSiD, CAS 1334032-16-4

UV-Vis-NIR Absorption


pbbtsid un-vis-nir absorption in chloroform
UV-Vis-NIR absorption of PBBTSiD in chloroform.

MSDS Documentation


PBBTSiD MSDSPBBTSiD MSDS sheet

Literature and Reviews


  1. Ambipolarity in Benzobisthiadiazole-Based Donor–Acceptor Conjugated Polymers, J. D. Yuen et al., Adv. Mater., 23, 3780–3785 (2011); DOI: 10.1002/adma.201101134.
  2. Organic Transistors in the New Decade: Toward n-Channel, Printed, and Stabilized Devices, S. Kola et al., J. Polym. Sci. B: Polym. Phys., 50, 1090–1120 (2012); DOI: 10.1002/polb.23054.
  3. Benzothiadiazole and its π-extended heteroannulated derivatives: useful acceptor building blocks for high-performance donor–acceptor polymers in organic electronics, Y. Wang et al., J. Mater. Chem. C, 4, 6200 (2016); DOI: 10.1039/c6tc01860b.

Return to the top