PNDI-T10, polymer acceptor for high-efficiency all-PSCs and OFETs

High purity polymer with high electron mobility


Specifications | MSDS | Literature and Reviews


PNDI-T10 (also known as PCE9), CAS number 1977539-03-9, is a polymer acceptor used in high-efficiency all-polymer solar cells (all-PSCs) and organic field-effect transistors (OFETs).

PNDI-T10 is a family member of polynaphthalene diimide (which is a copolymer of naphthalene diimide with bithiophene and thiophene unit.)

All-PSCs have received great research interest in recent years. This is thanks to the blend of both electron donor and acceptor being polymers in the active layer, and how having complementary absorption covers a wider range of the solar spectrum. Using polymer acceptors (instead of fullerene) in all-PScs also has the advantages of greater morphological stability, superior mechanical properties, and higher capability of being processed with ink-jet printing techniques in flexible devices.

PNDI-T10 has been successfully used in ternary all-PSCs, achieving record performances with PCE of 9% [1]. PNDI-T10 is also a potential candidate for high performance OFET with high electron mobility.

Luminosyn™ PNDI-T10


Luminosyn™ PNDI-T10 is now available.

High molecular weight and high purity

PNDI-T10 is purified by Soxhlet extraction with methanol, hexane and chlorobenzene under an argon atmosphere

Large quantity orders

Plan your experiments with the confidence of polymers from the same batch

General Information


Full name Poly{{[N,N'-bis(2-octyldodecyl)naphthalene-1,4,5,8-bis(dicarboximide)-2,6-diyl]-alt-5,5'-(2,2'-bithiophene)}-ran-{[N,N'-bis(2-octyldodecyl)naphthalene-1,4,5,8-bis(dicarboximide)-2,6-diyl]-alt-2,5-thiophene}}
Synonyms PCE9, PNDI-Th10, PNDI(2OD)-T10
Chemical formula (C62H88N2O4S2)0.9 ▪ (C58H86N2O4S)0.1
CAS number 1977539-03-9
HOMO / LUMO HOMO = -6.40 eV, LUMO = -4.10 eV [1]
Classification / Family PNDI polymers, Organic n-type semiconducting materials, PNDI polymers, Organic photovoltaics, All Polymer solar cells (all-PSCs), Electron-acceptor polymers, OFETs, Perovskite solar cells.
Soluble in Chloroform, chlorobenzene, dichlorobenzene
Recommended Processing Solvents at 10mg/ml Chloroform

Batch Details


Batch Mw PDI Stock Info
M2086A1 189,514 2.40 Discontinued
M2086A2 103,047 2.08 In stock

Chemical Structure


pndi-t10, 1977539-03-9
Chemical structure of PNDI-T10, CAS 1977539-03-9

MSDS Documentation


PNDI-T10 MSDSPNDI-T10 MSDS sheet

Literature and Reviews


  1. 9.0% power conversion efficiency from ternary all-polymer solar cells, Z. Li et al., Energy Environ. Sci., 10, 2212 (2017); DOI: 10.1039/c7ee01858d.
  2. High Performance All-Polymer Solar Cells by Synergistic Effects of Fine-Tuned Crystallinity and Solvent Annealing, Z. Li et al., J. Am. Chem. Soc., 138 (34), 10935–10944 (2016); DOI: 10.1021/jacs.6b04822.
  3. Energy-​effectively printed all-​polymer solar cells exceeding 8.61​% efficiency, Y. Lin et al., Nano Energy 46, 428-435 (2018); https://doi.org/10.1016/j.nanoen.2018.02.035.

Return to the top