PBQx-TF, high efficiency narrow bandgap copolymer

Single junction non-fullerene polymer PBQx-TF solar cells gives efficiency of close to 19%


Specifications | MSDS | Literature and Reviews


PBQx-TF is a highly efficient semiconducting polymer donor based on electron donating benzo[1,2-b:4,5-b']dithiophene (BDT) and electron withdrawing dithieno[3,2-f:2',3'-h]quinoxaline (DTQx) units as the main backbone, bearing two 2-ethylhexyl-3-fluorothiophene side chains on the fused BDT ring and 2-butyloctyl solubilising groups on the bridging thiophen rings.

Single junction non-fullerene polymer solar cells based on PBQx-TF as the electron donor and eC9-2Cl:F-BTA3 as the binary electron acceptors in the active layer achieved a PCE of 19% with an open-circuit voltage of 0.879 V, short-circuit current density of 26.7 mA cm-2, and fill factor of 0.809. The device had the following structure [1].

Device structure: ITO/PEDOT:PSS AI 4083/PBQx-TF:eC9-2Cl:F-BTA3 (1:1:0.2)/PNDIT-F3N-Br/Ag

Thickness (nm) VOC (V) JSC (mA cm-2) FF (%) PCE (%)
100 0.879 26.7 80.9 18.99

For 5 – 10 grams order quantity please contact us for details, the lead time is 4 – 6 weeks.

Luminosyn™ PBQx-TF (PCE19)


Luminosyn™ PBQx-TF is now available.

High purity

PBQx-TF is purified via Soxhlet extraction with acetone, hexane, and chlorobenzene under an argon atmosphere

Large quantity orders

Plan your experiments with polymers from the same batch

General Information


CAS Number N/A
Chemical Formula (C78H94F2N2S8)n
Full Name Poly[(2,6-(4,8-bis(5-(2-ethylhexyl)-4-fluoro)thiophen-2-yl)-benzo[1,2-b:4,5-b’]dithiophene)-alt-5,5'-(6,9-bis(4-(2-butyloctyl)thiophen-2-yl)dithieno[3,2-f:2',3'-h]quinoxaline)]
HOMO / LUMO HOMO = -5.41 eV, LUMO = -2.82 eV [1]
Solubility Chloroform, chlorobenzene and dichlorobenzene
Recommended Processing Solvents at 10mg/ml o-Xylene (8mg/ml - M2383A1), dichlorobenzene (5mg/ml - M2383A2)
Synonyms PCE19
Classification / Family Organic semiconducting materials, Medium bandgap polymers, Organic photovoltaics, Polymer solar cells, Perovskite solar cells, Hole-transport layer materials, NF-PSCs, All-polymer solar cells (all-PSCs)

Batch Details


Batch Mw Mn PDI Stock Info
M2383A1 40,126 16,342 2.46 In stock
M2383A2 119,668 33,168 3.61 In stock

Chemical Structure


PBQx-TF chemical structure
Chemical structure of PBQx-TF, Poly[(2,6-(4,8-bis(5-(2-ethylhexyl)-4-fluoro)thiophen-2-yl)-benzo[1,2-b:4,5-b’]dithiophene)-alt-5,5'-(6,9-bis(4-(2-butyloctyl)thiophen-2-yl)dithieno[3,2-f:2',3'-h]quinoxaline)]

MSDS Documentation


PBQx-TF MSDSPBQx-TF MSDS Sheet

Literature and Reviews


  1. Single-Junction Organic Photovoltaic Cell with 19% Efficiency, Y. Cui et al., Adv. Mater., 33 (41), 2102420 (2021); DOI: 10.1002/adma.202102420.
  2. A chlorinated lactone polymer donor featuring high performance and low cost, K. Jin et al., J. Semicond., 43, 050501 (2022); DOI: 10.1088/1674-4926/43/5/050501.
  3. Star polymer donors, J. Cao et al., J. Semicond., 43, 070201 (2022); DOI: 10.1088/1674-4926/43/7/070201.