IDT-2Br, NFA with excellent thermal stability and a strong, broad absorption

High purity (≥98%) and able to give device performances of up to 12.1% efficiency


Specifications | Pricing and Options | MSDS | Literature and Reviews


IDT-2Br (CAS number 2042521-91-3), like o-IDTBR, has an electron-donating ladder-type fused five-member-ring indaceno[1,2-b:5,6-b′]dithiophene (IDT) core with 4-hexylphenyl side chains, flanked by two electron withdrawing benzothiadiazole moieties and rhodanine terminated groups.

IDT-2Br is a planar electron acceptor when it is compared with o-IDTBR, exhibiting excellent thermal stability, strong and broad absorption, relatively high electron mobility.

When PTB7-Th was used as the low band-gap donor polymer, mixed acceptors of F8IC and IDT-2Br demonstrated a great device performance with 12.1% efficiency

High efficient non-flullerene acceptor

High efficient non-fullerene acceptor

with highly conjugated core

Planar molecular configuration

Planar molecular configuration

Excellent thermal stability, broad absorption and high electron mobility

Worldwide shipping for 2042521-91-3

Worldwide shipping

Quick and reliable shipping

High purity

High purity

>99% High purity

Device structure: indium tin oxide (ITO)/ zinc oxide (ZnO)/PCE10:IDT-2BR:F8IC/molybdenum oxide (MoO3)/Ag [2]

Thickness (nm) VOC (V) JSC (mA cm-2) FF (%) PCE (%)
100 nm 0.687 25.1 69.9 12.1

Chemical Structure

Chemical structure of IDT-2Br
Chemical structure of IDT-2Br, CAS number: 2042521-91-3

General Information


CAS Number 2042521-91-3
Chemical Formula C88H88N6O2S8
Purity ≥98% (1H NMR)
Full Name 5,5'-[[4,4,9,9-Tetrakis(4-hexylphenyl)-4,9-dihydro-s-indaceno[1,2-b:5,6-b']dithiophene-2,7-diyl]bis(2,1,3-benzothiadiazole-7,4-diylmethylidyne)]bis[3-ethyl-2-thioxo-4-thiazolidinone]
Molecular Weight 1518.20 g/mol
Absorption λmax 636 nm (Chloroform); λmax 658 nm (Film)
HOMO / LUMO HOMO = -5.52 eV, LUMO = -3.69 eV [1]
Melting Point TGA 367 °C (5% weight loss) (lit.)
Solubility Chloroform, chlorobezene
Form Dark blue powder/crystals
Synonyms IDT2BR
Classification / Family NFAs, n-type non-fullerene electron acceptors, Organic semiconducting materials, Low band-gap small molecule, Small molecular acceptor, Organic photovoltaics, Polymer solar cells, NF-PSCs.

Pricing


Batch Quantity Price
M2252A1 100 mg £320
M2252A1 250 mg £640
M2252A1 500 mg £1150
M2252A1 1 g £2100
M2252A1 5 g / 10 g* Please contact us for details

*for 5 - 10 grams order quantity, the lead time is 4 - 6 weeks

MSDS Documentation


o-IDTBR MSDSIDT-2BR MSDS Sheet

Literature and Reviews


  1. A planar electron acceptor for efficient polymer solar cells, Y. Wu et al., Energy Environ. Sci., 8, 3215-3221 (2015); doi: 10.1039/C5EE02477C.
  2. High-performance ternary organic solar cells with photoresponses beyond 1000 nm, P. Xue et al., J. Mater. Chem. A, 6, 24210-24215 (2018); doi: 10.1039/C8TA09042D.

Related Products


Non-Fullerene Acceptors Collection

Non-Fullerene Acceptors

Non-Fullerene Acceptors

Non-fullerene acceptors (NFAs) are a promising alternative to fullerene-based electron acceptors.

Semiconducting Polymers Collection

Semiconducting Polymers

Semiconducting Polymers

Semiconducting polymers for bulk heterojunction, OPV, OLED, OFET and perovskite interfaces and solar cell research.

Organic Conductors Collection

Organic Conductors

Organic Conductors

Organic conductors are an environmentally friendly alternative to traditional inorganic conductors.

Return to the top