Product Code C202-X10
Price $129

High-precision micro cleaning swabs

High-precision & Standard types available


High-precision micro cleaning swabs for fine cleaning and standard swabs for general cleaning, made and packaged in a Class 10000 cleanroom. The head is thermally bonded to the body, avoiding the use of glue or solvents. This decreases the possibility of contamination and minimal particle shedding.

Sharp and narrow High-precision Clean room Swabs

High-precision (C201)

Standard Clean room Swabs

Standard (C202)

 

High-precision (C201) Standard (C202)
Body Clean room paper Plastic tube
Head Compressed cotton Compressed cotton
Type Double headed Double headed
Handle length 55 mm 50 mm
Handle thickness 1.5 mm 3.0 mm
Head width 3 mm (with pointed tip) 4 mm
Head length 12 mm 12 mm
Pack Sizes 25 and 100 100 and 1000