Product Code M2400B1-50g
Price $108

Hydrophilic γ-Al2O3 nanoparticles with ~ 18 nm ave. particle size, >99.5% purity

High purity gamma-phase aluminum oxide powders for application as catalysts, in water treatment, organic electronics and more.


Technical Data | MSDS | Literature and Reviews


Aluminum oxide (Al2O3, CAS number 1344-28-1), known as alumina, is one of the most frequent metal oxides used in industry due to its abundance in nature and low-cost production. Alpha (α), Beta (β) and gamma (ƴ) are the most well-known phase modifications of aluminum oxide.

γ-Al2O3 is used as a carrier of catalysts and a desiccant in processes of chemical and petrochemical production owing to its high surface area with open porosity and relatively stable over the temperature range of interest for most catalytic reactions. Aluminum oxide nanoparticles can also serve as additives to concrete mixtures, cosmetics, and textile industries. Aluminum oxide nanoparticles have also been used as antibacterial agent for biomedical purposes. Owing to its electrical resistance, aluminum oxide scaffold is beneficial for suppressing charge recombination, preventing moisture penetration, and increasing the thickness of light absorber layer in perovskite solar cells.

Alumina nanoparticles, mainly in α-and γ-forms, have been widely applied in adsorption-based applications because of their interesting properties such as high specific surface area (SSA), mechanical and thermal stability, inertness to most acids and alkalis, good electrical and chemical resistance in both oxidizing and reducing atmospheres up to 1000 °C, electrical insulation, high melting points, as well as being non-toxic and low-cost.

High purity aluminum Oxide

High purity

>99.5% purity

Worldwide shipping

Worldwide shipping

Quick and reliable shipping

high specific surface area

High SSA

~ 18 nm Particle size 140 m2/g SSA

Mechanical and Thermal stability

Mechanical & Thermal stability

Stable over a wide temperature range

Technical Data


CAS Number 1344-28-1
Chemical Formula Al2O3
Molecular Weight 101.96 g/mol
Chemical Name Aluminum oxide
Synonyms Alumina, Aluminium oxide
Classification / Family 2D semiconducting materials, nanomaterials, Solid lighting, metal oxides
Colour White powder

Product Information


Product Code M2400A1 M2400B1
Average Particle Size ~ 18 nm 20 nm
Specific Surface Area 140 m2/g N/A
Specific Heat Capacity 890 J/kg K N/A
True Density 3.9 g/cm3 N/A
Melting Point 2040 °C (lit.) 2040 °C (lit.)
Purity > 99.5% ≥ 99.99%

*For larger orders please contact us to discuss prices

MSDS Documents


aluminum oxide (Al2O3) nanoparticles MSDSAluminum Oxide Powders MSDS Sheet

Literatures


  1. Preparation of γ-Al2O3 nanoparticles using modified sol-gel method and its use for the adsorption of lead and cadmium ions, J. Alloys Compd., S. Tabesh et al., 730, 441-449 (2018); DOI: 10.1016/j.jallcom.2017.09.246.
  2. Cr3+ doped Al2O3 nanoparticles: Effect of Cr3+ content in intensifying red emission, P. Lewis et al., Curr. Appl. Phys., 32, 71-77 (2021); DOI: 10.1016/j.cap.2021.10.003.
  3. A novel foam formulation by Al2O3/SiO2 nanoparticles for EOR applications: A mechanistic study, H. Rezvani et al., J. Mol. Liq., 304, 112730 (2020); DOI: 10.1016/j.molliq.2020.112730.

Return to the top