It looks like you are using an unsupported browser. You can still place orders by emailing us on info@ossila.com, but you may experience issues browsing our website. Please consider upgrading to a modern browser for better security and an improved browsing experience.


Product Code M1201A4-100mg
Price $540

P(NDI2OD-T2), electron acceptor in polymer solar cells

High mobility n-type polymer semiconductor available online for priority dispatch


Overview | Specifications | MSDS | Literature and Reviews


PNDI(2OD)2T (CAS number 1100243-40-0), a copolymer of naphthalene diimide (NDI) and bithiophene unit, has been intensively studied for use as an electron acceptor in polymer solar cells. This is due to its high electron mobility, high electron affinity, and broad light absorption. All polymer solar cells with PNDI(2OD)2T as an acceptor and J51 as a donor (fullerene-free) have demonstrated a power conversion efficiency over 8% [1].

PNDI(2OD)2T is also known as a high-mobility n-type polymer semiconductor. PNDI(2OD)2T-based OFET devices have electron mobilities up to 0.45–0.85 cm2V-1 s-1[2].

PNDI(2OD)2T from Ossila was used in a high-impact paper (IF 18.81)

PNDI(2OD)2T from Ossila was used in the high-impact paper (IF 18.81), Tuning Contact Resistance in Top-Contact p-Type and n-Type Organic Field Effect Transistors by Self-Generated Interlayers, T. Sarka et al., Adv. Funct. Mater., 1805617 (2020); DOI: 10.1002/adfm.201805617.

Luminosyn™ PNDI(2OD)2T


Luminosyn™ PNDI(2OD)2T is now available.

High molecular weight and high purity

PNDI(2OD)2T is purified by Soxhlet extraction with methanol, hexane and chlorobenzene under an argon atmosphere

Batch-specific GPC data

Have confidence in what you are ordering; batch-specific GPC data for your thesis or publications

Large quantity orders

Plan your experiments with confidence with polymers from the same batch

General Information


Full name Poly{[N,N'-bis(2-octyldodecyl)naphthalene-1,4,5,8-bis(dicarboximide)-2,6-diyl]-alt-5,5'-(2,2'-bithiophene)}
Synonyms
  • P(NDI2OD-T2)
  • PNDI-2T
  • Polynaphtalene-bithiophene
  • N2200
Chemical formula (C62H88N2O4S2)n
CAS number 1100243-40-0
HOMO / LUMO HOMO = -5.77 eV, LUMO = -3.84 eV [1]
Classification / Family PNDI polymers, Organic n-type semiconducting materials, Organic photovoltaics, Polymer solar cells, Electron-acceptor polymers, OFETs, Perovskite solar cells.
Soluble in Chloroform, chlorobenzene, dichlorobenzene
Recommended Processing Solvents at 10mg/ml Chloroform

Batch Details


Batch number MW Mn PDI Stock info
M1201A4 186,027 90,949 2.05 In Stock

Chemical Structure


chemical structure of P(NDI2OD-T2)
Chemical structure of PNDI(2OD)2T

MSDS Documentation


PNDI(2OD)2T MSDSPNDI(2OD)2T MSDS sheet

Literature and Reviews


  1. All-Polymer Solar Cells Based on Absorption-Complementary Polymer Donor and Acceptor with High Power Conversion Efficiency of 8.27%, L. Gao et al., Adv. Mater., 28, 1884–1890 (2016); DOI: 10.1002/adma.201504629.
  2. A high-mobility electron-transporting polymer for printed transistors, H. Yan et al., Nature, 457 (2009); doi:10.1038/nature07727.
  3. Highly efficient charge-carrier generation and collection in polymer/polymer blend solar cells with a power conversion efficiency of 5.7%, D. Mori et al., Energy Environ. Sci., 7, 2939-2943 (2014); DOI: 10.1039/C4EE01326C.