PFO-co-MEH-PPV, CAS number 1383605-56-8, is a co-polymer consisting of alternating 9,9-dioctylfluorenyl and 2-methoxy-5-(2-ethylhexyloxy)-1,4- phenylenevinylene (MEH-PPV) repeating units in its main backbone structure.

Owing to its capability of harvesting the energy from non-emissive triplet states, PFO-co-MEH-PPV is a reverse intersystem crossing (RISC) polymer which can be used in solution processable, non-doped, highly efficient OLED devices.

PFO-co-MEH-PPV can also be used for polymer lasers with the demonstration of a relaxation oscillation and a picosecond pulse generation.

General Information


CAS number 1383605-56-8
Chemical formula (C48H66O2)n
Absorption* λmax 480 nm (in toluene)
Fluorescence λmax 550 nm (in film)
HOMO/LUMO HOMO = 4,4 eV, LUMO = 2.1 eV [1]
Full name
Poly[{9,9-dioctyl-2,7-divinylene-fluorenylene}-alt-co-{2-methoxy-5-(2-ethylhexyloxy)-1,4-phenyene}]
Synonyms PFOPV, PFPV, PEPV
Solubility Toluene, chloroform or chlorobenzene
Classification / Family PFO and PPV derivatives, Hole transport layer materials; Polymer light-emitting diodes (OLEDs), Green emitter, Organic photovoltaics (OPVs), Polymer lasers, Organic electronics

* Measurable with an optical spectrometer

Product Details

Purity >99%
Thermogravimetric Analysis (TGA) n.a.
Appearance Bright yellow powder/fiber

Chemical Structure

Chemical structure of PFO-co-MEH-PPV
Chemical structure of PFO-co-MEH-PPV

Pricing


Batch Quantity Price
M2196A 100 mg £260
M2196A 250 mg £520
M2196A 500 mg £830

Batch information


Batch Mw Mn PDI Stock info
M2196A1 302 kDa
131 kDa 2.3 Discontinued
M2196A2 150 kDa


Low stock
M2196A3 80 kDa 35 kDA 2.3 In stock

MSDS Documentation


PFO-co-MEH-PPV MSDSPFO-co-MEH-PPV MSDS sheet

Literature and Reviews


  1. The Triplet-Charge Annihilation in Copolymer-Based Organic Light Emitting Diodes: Through “Scattering Channel” or “Dissociation Channel”?, D. Yuan et al., Phys. Chem. Chem. Phys., 17, 27609-27614 (2015); 10.1039/C5CP05016B.
  2. Relaxation Oscillation with Picosecond Spikes in a Conjugated Polymer Laser, W. Mujamammi et al., Polymers 8, 364 (2016); doi:10.3390/polym8100364
  3. Advances in Conjugated Polymer Lasers, H. Xia et al, Polymers, 11, 443 2019); doi: 10.3390/polym11030443.

Return to the top