PFN-Br, used to improve extraction efficiencies in organic electronic devices

High quality polymer available for fast, secure dispatch


Overview | Specifications | Pricing and Options | MSDS | Literature and Reviews


With hydrophobic backbone and hydrophilic side chains, PFN-Br (CAS number 889672-99-5) is a conjugated polymer electrolyte (CPE). It serves as an electron-interface layer material in organic electronic devices (including OFET, OLED, OPV and perovskite solar cells) to improve the interfacial properties such as extraction efficiency.

PFN-Br interfacial layer embedded in OPV devices gives overall enhanced open-circuit voltage, short-circuit current density and fill factor thus improved device performance. It is also believed that the device performance of polymer LEDs with bilayer cathodes (e.g. PFN-Br/Al), can be enhanced to levels comparable to (and even higher than) those obtained from using Ca or Ba cathodes due to its strong polar ionic pendant groups.

Cathode interlayer molecule

Cathode interlayer molecule

For high efficient OPV applications

Improve extraction efficiency

Improve extraction efficiency

as a conjugated polyelectrolyte

Worldwide shipping for 889672-99-5

Worldwide shipping

Quick and reliable shipping

enhance the device performance of polymer LEDs

Enhance device performance

strong polar ionic pendant groups

PFN-Br has been used in highly efficient OPV tandem structures with device efficiency over 17%.

General Information


Full name Poly(9,9-bis(3’-(N,N-dimethyl)-N-ethylammoinium-propyl-2,7-fluorene)-alt-2,7-(9,9-dioctylfluorene))dibromide
Synonyms
  • PFN-bromide
  • PFNBr
Chemical formula (C56H80N2Br2)n
CAS number 889672-99-5
Classification/Family Conjugated polymers, Polymer electrolyte, Polyfluorenes, Electron interface layer materials, OLED, OPV, Perovskite materials

Chemical Structure


pfn-br, pfnbr structure
Chemical structure of PFN-Br, CAS# 889672-99-5.

Batch information


Batch Mw Mn PDI Stock info
M2230A1 165 kDa 57 kDa 2.9 Discontinued
M2230A2 190 kDa 61 kDa 3.1 Discontinued
M2230A3 84 kDa 40 kDa 2.1 Discontinued
M2230A4 131 kDa 42 kDa 3.1 In Stock

Pricing


Batch Quantity Price
M2230A 100 mg £280
M2230A 250 mg £560
M2230A 500 mg £950

MSDS Documentation


PFN-Br MSDSPFN-Br MSDS sheet

Literature and References


  1. Efficient Electron Injection from a Bilayer Cathode Consisting of Aluminum and Alcohol-/Water-Soluble Conjugated Polymers, H. Wu et al., Adv. Mater., 16, 1826–1830 (2004), DOI: 10.1002/adma.200400067.
  2. High-Performance Polymer Solar Cells Based on a Wide Bandgap Polymer Containing Pyrrolo[3,4- f]benzotriazole5,7-dione with a Power Conversion Efficiency of 8.63%, L. Lan et al., Adv. Sci., 3, 1600032 (2016); DOI: 10.1002/advs.201600032.
  3. Toward high performance inverted polymer solar cells, X. Gong et al., Polymer 53, 5437e5448 (2012); DOI: 10.1016/j.polymer.2012.09.023.

Return to the top