Product Code M2405A1-50g
Price $180

NMC811, Nickel-Rich Layered LiNi0.8Mn0.1Co0.1O2 Powder, Battery Cathode Materials

Low cost high specific energy capacity as lithium-ion battery cathode material for electrical vehicles


Technical Data | MSDS | Literature and Reviews | Related Products


Lithium nickel manganese cobalt oxide (NMC811), CAS number 179802-95-0, is considered one of the most promising future cathode materials for lithium-ion batteries in electric vehicles due to its high specific energy density, favourable rate capability and relatively low product cost. NMC811 delivers a high specific capacity of ~200 mAh g-1 with a moderately high average discharge potential of ~3.8 V vs Li+/Li, a substantial increase of ~25% in energy density compared to that of LiCoO2.

NMC811 adopts the well-known α−NaFeO2 type layered oxide (R3m) structure characterized by a close-packed oxygen lattice and alternating layers of lithium and transition metal ions reside at the centre in octahedral coordination environments.

Electrochemical fluorination enhances the cycling stability of the electrode without altering bulk structure and morphology. ECF-NMC811 cathodes delivered 203.0 mA h g-1 first discharge capacity at the current rate of C/10, with ~98% capacity retention up to 100 cycles.

high specific energy density 179802-95-0

High specific energy density

Promising future cathode material

low cost Lithium Nickel Manganese Cobalt Oxide

Low cost

Low Product cost

versatile 179802-95-0

versatile

Ideal candidate for EVs, power tools, and grid energy storage.

Quick Worldwide shipping

Worldwide shipping

Quick and reliable shipping

Technical Data


CAS Number 179802-95-0
Chemical Formula LiNi0.8Mn0.1Co0.1O2
Molecular Weight 97.28 g/mol
Chemical Name Lithium Nickel Manganese Cobalt Oxide
Synonyms NMC811, NCM811
Classification / Family 2D semiconducting materials, Battery materials, Metal oxides, Cathode materials
Colour Black to grey powder

Lithium Nickel Manganese Cobalt Oxide Powder


Product Code M2405A1
Li 7.00%
Co + Mn +Ni 59.0%
Li2CO3 0.35%
LiOH 0.35%
BET ≤0.60 m2/g
Tap Density 2.2 m2/g
Compact Density 3.4 g/cm3
Particle Size ~8.0 – 13 µm
pH ≤12

*For larger orders please email us to discuss prices.

MSDS Documents


lithium nickel manganese cobalt oxide (NMC811) powder MSDSLithium Nickel Manganese Cobalt Oxide (NMC811) Powder MSDS Sheet

Literatures


  1. The effects of ambient storage conditions on the structural and electrochemical properties of NMC-811 cathodes for Li-ion batteries, C. Busà et al., Electrochim. Acta, 366, 137358 (2021); DOI: 10.1016/j.electacta.2020.137358.
  2. Enhancing Cycling Stability and Capacity Retention of NMC811 Cathodes by Reengineering Interfaces via Electrochemical Fluorination, B. Thapaliya et al., Adv. Mater. Interfaces, 9(18), 2270102 (2022); DOI:10.1002/admi.202270102.
  3. Identifying the Origins of Microstructural Defects Such as Cracking within Ni-Rich NMC811 Cathode Particles for Lithium-Ion Batteries, T. Heenan et al., Adv. Energy Mater., 10, 2002655 (2020); DOI: 10.1002/aenm.202002655.


We stock a wide range of Battery Materials available to purchase online. Please contact us if you cannot find what you are looking for.

Cathode Active Materials Collection

Cathode Active Materials

Cathode Active Materials

Explore the range of high-purity cathode materials including NMC and LCO

Metal Oxide Collection

Metal Oxides

Metal Oxides

A range of metal oxides for application in batteries and much more.

Anode Active Materials Collection

Anode Active Materials

Anode Active Materials

Explore the range of anode active materials including graphite.

Technical Support


Contact Ossila

To find out more, complete the form below to contact our technical team directly. You can also email info@ossila.com to request a quote or place an order.

Please fill the field
Please enter valid email address
Please enter your message
Return to the top