Sublimed Eu(dbm)3(Phen), >99.0% purity

Red-orange phosphorescence emitter, Tris(dibenzoylmethane)phenanthroline europium(III), CAS No. 17904-83-5, Sublimed ≥99.0%


Eu(dbm)3(Phen) is a typical tenary Eu3+complex with a ligand 1,3- diphenylpropane-1,3-dione and a secondary phenanthroline ligand coordinating to the europium core. Eu(dbm)3(Phen) displays red-orange phosphorescence emission at 615 nm with a narrow bandwidth (color purity) FWHM smaller than 100 cm-1 in OLEDs. Eu(dbm)3(Phen) is preferably co-deposited with a charge transport material to reduce the chance of self-quenching (concentration quenching) and to improve charge carrier mobilities.

Eu(dbm)3(Phen) is also frequently embedded in polyvinylcarbazole (PVK) or mesoporous silica nanoparticles for electroluminescence studies to improve its efficiency and photo stability.

General Information


CAS number 17904-83-5
Full name Tris(dibenzoylmethane)phenanthroline europium(III)
Chemical formula C57H41N2O6Eu
Molecular weight 1001.93 g/mol
Absorption λmax 257 nm, 355 nm in THF
Fluorescence λem 615 nm in THF
HOMO/LUMO HOMO = 5.22 eV, LUMO = 2.93 eV [1]
Synonyms Tris(dibenzoylmethane) mono(1,10-phenanthroline)europium(lll)
Classification / Family Europium complexes, Organic electronics, Red dopant, Sublimed materials.

Product Details


Purity Sublimed: >99.0% (HPLC)
Melting point Mp (onset) =199°C (DTA), TGA: 234.6 °C (0.5% weight loss)
Appearance Yellow powder/crystals

*Sublimation is a technique used to obtain ultra pure-grade chemicals. For more details about sublimation, please refer to the Sublimed Materials.

Chemical Structure


Eu(dbm)3(Phen), 17904-83-5
Chemical structure of Tris(dibenzoylmethane)phenanthroline europium(III) - Eu(dbm)3(Phen), CAS 17904-83-5

Device Structure(s)


Device structure ITO/PEDOT:PSS/TAPC (50 nm)/PVK:20 wt% Eu(dbm)3(Phen)/b-PBD/Al [2]
Colour red light emitting device Pinkish-Red
Luminous efficiency@29 V 26 cd/mA

*For chemical structure information, please refer to the cited references.

Pricing


Grade Order Code Quantity Price
Sublimed (>99.0% purity) M2296A1 250 mg £330
Sublimed (>99.0% purity) M2296A1 500 mg £520
Sublimed (>99.0% purity) M2296A1 1 g £850

MSDS Documentation


Eu(dbm)3(Phen) MSDSEu(dbm)3(Phen) MSDS sheet

Literature and Reviews


  1. Preparation and characteristics of Eu(DBM)3phen: Synthesis, single-crystal structure and spectroscopic analysis, L. Ruan et al., J. Mol. Struct., 1149, 265-272 (2017); DOI: 10.1016/j.molstruc.2017.08.003.
  2. The dependence of OLED external efficiency on the mass concentration of europium(III) dispersed in PVK, G. Santos et al., ECS Trans., 39 (1), 475-480 (2011); DOI:10.1149/1.3615229.
  3. Optical amplification of Eu(DBM)3Phen-doped polymer optical fiber, H. Liang et al., Opt. Lett., 29 (6), 447-449 (2004); DOI:10.1364/OL.29.000477.