AI 4083 PEDOT:PSS

CAS Number 155090-83-8

Materials, Organic Conductors, PEDOT Polymer Blends

Product Code M121-100ml
Price $334

Popular Aqueous PEDOT:PSS Formulation

Used for applications in OPV, OLED, perovskite solar cells, and lighting


Specifications | MSDS | Resources and Support


P VP AI 4083 (CAS number 155090-83-8) is one of the most commonly used aqueous PEDOT:PSS formulations. Due to its deep work function it is often used for the matching of interfacial energy levels in thin film electronic devices. With a PEDOT:PSS ratio of 1:6, AI 4083 has low conductivity with relatively high resistance of 500 to 5000 Ω.cm. It has been widely used in organic and inverted PSCs and OLEDs as a hole transport material.

Deep Work Function PEDOT

Deep Work Function

Matching interfacial energy levels

Versitle use in OPV, OLED and perovskite solar

Versatile Use

OPV, OLED, and perovskite solar cells

High quality PEDOT

High Quality

Quality assured material

Low Conductivity PEDOT

Low Conductivity

Tailored low conductivity

PEDOT:PSS from Ossila was featured in the high-impact paper (IF 30.85)

PEDOT:PSS (AI 4083) from Ossila was featured in the high-impact paper (IF 56.7), Scalable two-terminal all-perovskite tandem solar modules with a 19.1% efficiency, B. Nejand et al., Nat. Energy, 7, 620–630 (2022): DOI: 10.1038/s41560-022-01059-w; and paper (IF 9.5), Benzophenone: A Small Molecule Additive for Enhanced Performance and Stability of Inverted Perovskite Solar Cells, H. Elbohy et al., ACS Appl. Mater. Interfaces, 15 (38), 45177–45189 (2023); DOI: 10.1021/acsami.3c09835.

Technical Data


Product Name Clevios™ P VP AI 4083
Solvent Water
Composition PEDOT/PSS (1:6 w/w)
CAS Number 155090-83-8
Solid Content 1.3 – 1.7 wt.%
Work Function 5.0 – 5.2 eV
Resistivity 500 – 5000 Ω.cm
Sheet Resistance +10E6 Ω/sq
Conductivity Low conductivity, 0.0002 – 0.002 S/cm
Particle Size Distribution D90 = 100 nm; D50 = 80 nm
Viscosity 5 – 12 mPa.s
pH Value 1.0 – 2.0
Packaging 100 ml of solution sealed in a light resistant bottle with temperature indicator
Storage 3 – 5 °C

Spin Speed Data


Al 4083 Spin Speed / Film ThicknessAl 4083 Spin Speed / Film Thickness

MSDS Document


Al 4083 MSDS SheetAl 4083 PEDOT:PSS MSDS Sheet

Related Products


Resources and Support


PEDOT:PSS Deposition How to Spin Coat PEDOT:PSS

For the deposition of thin films of PEDOT:PSS on a freshly prepared surface, we recommend using a vacuum-free spin coater and following this five-step process:

Read more...
PEDOT and PEDOT:PSS Synthesis PEDOT and PEDOT:PSS Synthesis

PEDOT synthesis involves the oxidative chemical or electrochemical polymerization of EDOT monomer. The choice of counterions and polymerization method significantly affects the conductivity, work function, and stability of the resulting PEDOT polymer.

Read more...
Return to the top