It looks like you are using an unsupported browser. You can still place orders by emailing us on info@ossila.com, but you may experience issues browsing our website. Please consider upgrading to a modern browser for better security and an improved browsing experience.
UGH2, ETL and HBL material for organic electronic devices
TADF host material for blue-emitting dopants in highly-efficient blue PhOLEDs, CAS No. 40491-34-7 / 18856-08-1, Sublimed ≥99.0%
1,4-Bis(triphenylsilyl)benzene, known as UGH-2, is one of the well-known TADF host materials for blue-emitting dopants (such as FIrPic) in highly-efficient blue PhOLEDs. This is due to its wide energy gap (4.4 eV) and high triplet energy (ET = 3.5 eV).
With a very deep HOMO energy level (HOMO = 7.2 eV), UGH-2 also works as an electron-transport (ETL) and hole-blocking layer (HBL) material.
General Information
CAS number
40491-34-7; 18856-08-1
Full name
1,4-Bis(triphenylsilyl)benzene
Chemical formula
C42H34Si2
Molecular weight
594.89 g/mol
Absorption
λmax 265 nm in DCM
Fluorescence
λem 298 nm in DCM
HOMO/LUMO
HOMO = 7.2 eV, LUMO = 2.8 eV (ET = 3.5 eV)
Synonyms
UGH2, 1,4-Phenylenebis(triphenylsilane)
Classification / Family
Organic electronics, Hole-blocking layer materials (HBL), TADF blue host materials, Blue PhOLEDs, TADF-OLEDs, Sublimed materials.
Product Details
Purity
Sublimed: >99.0% (HPLC)
Melting point
TGA: >270 °C (0.5% weight loss)
Colour
White powder/crystals
*Sublimation is a technique used to obtain ultra pure-grade chemicals, see the sublimed materials.
Chemical Structure
Chemical structure of UGH-2, CAS 40491-34-7 / 18856-08-1
High Efficiency White Organic Light-Emitting Devices Incorporating Yellow Phosphorescent Platinum(II) Complex and Composite Blue Host, S-L. Lai et al., Adv. Funct. Mater. 2013, 23, 5168–5176 (2013); DOI: 10.1002/adfm.201300281.
Iridium(III) Complexes of a Dicyclometalated Phosphite Tripod Ligand: Strategy to Achieve Blue Phosphorescence Without Fluorine Substituents and Fabrication of OLEDs, C-H. Lin et al., Angew. Chem., 123, 3240 –3244 (2011); DOI: 10.1002/ange.201005624 .
En Route to High External Quantum Efficiency (~12%), Organic True-Blue-Light-Emitting Diodes Employing Novel Design of Iridium (III) Phosphors, Y-C. Chiu et al., Adv. Mater., 21, 2221–2225 (2009); DOI: 10.1002/adma.200802546.
Deep-blue phosphorescent iridium complexes with picolinic acid N-oxideas the ancillary ligand for high efficiency organic light-emitting diodes, H-J. Seo et al., Org. Electron., 11, 564–572 (2010); doi: 10.1016/j.orgel.2009.12.014.
High efficiency blue phosphorescent organic light-emitting device, N. Chopra et al., Appl. Phys. Lett. 93, 143307 (2008); doi: 10.1063/1.3000382.
The Ossila website uses cookies for core functionality. By continuing to browse the website you consent to the use of these cookies.More Information
Online orders to can only be placed in . For other payment methods, request a quote or send a purchase order to info@ossila.com to purchase via offline channels.