Useful for a variety of experimental techniques including microscopy (STM, conductive AFM), spectroscopy and electropolymerisation.

 

Specifications

Substrate size 20 mm x 15 mm
Thickness 1.1 mm
Glass type Polished soda lime, float glass
Substrate coating Fully oxidized ITO
ITO thickness 100 nm
ITO resistance 20 Ω / square
Glass roughness 1 nm RMS (by AFM)
ITO roughness 1.8 nm RMS (by AFM)
Packaging Stacks of 20 separated by cleanroom paper

 

Characterisation

 

AFM scan of ITO substrateAFM of glass surface of ITO substrates
Left: 10 µm x 10 µm AFM scan with Z-scale of ±5 nm. Right: AFM of glass surface (1 µm x 1 µm x 3.5 nm). Courtesy of Richard T Grant.

 

Transmittance of ITO
Transmittance of ITO substrates.

 