POSTF


Product Code M2337A1
Price $376.00 ex. VAT

POSTF, namely 2'-(Diphenylphosphoryl)-10-phenyl-10H-spiro[acridine-9,9'-fluorene], has an orthogonal molecular structure with an electron donating spiro[acridine-9,9'-fluorene] core and one electron withdrawing diphenylphosphine oxide attachment to the fluorene unit at 2-poistion.

Bipolar POSTF can be used as a single or together with PO-T2T as an exciplex phosphorescent host for highly efficient blue, green and red phosphorescence devices. Using POSTF as the host, large-size white light-emitting panel (15 cm × 15 cm) with max power efficiency of 75.9 lm W-1 can be achieved [1].

General Information

CAS number 1647050-25-6
Full name 2'-(Diphenylphosphoryl)-10-phenyl-10H-spiro[acridine-9,9'-fluorene]
Chemical formula C43H30NOP
Molecular weight 607.68 g/mol
Absorption λmax 280 nm, 325 nm (in DCM)
Phosphorescene λmax 430 nm (in DCM)
HOMO/LUMO HOMO = 5.57 eV, LUMO = 2.12 eV [1]
Synonyms Diphenyl(10-phenyl-10H-spiro[acridine-9,9'-fluoren]-2'-yl)phosphine oxide
Classification / Family Spiro[acridine-9,9'-fluorene] derivatives, Light-emitting diodes, Bipolar host, TADF host materials, Sublimed materials.

Product Details

Purity Sublimed >99.0% (HPLC)
Melting point Tg = 160 ℃, Td (Temperature at 5% weight loss) = 356 ℃.
Appearance White powder/crystals

*Sublimation is a technique used to obtain ultra pure-grade chemicals. For more details about sublimation, please refer to the Sublimed Materials for OLED devices page.

Chemical Structure

POSTF chemical structure

Chemical structure of 2'-(Diphenylphosphoryl)-10-phenyl-10H-spiro[acridine-9,9'-fluorene] (POSTF), CAS# 1647050-25-6.

Device Structure(s)

Device structure ITO/HAT-CN (10 nm)/TAPC (45 nm)/POSTF: FIrpic (15 vol%, 20 nm)/TmPyPB (40 nm)/Liq (2 nm)/Al [1]
Colour Blue blue
Max. Power Efficiency 50.5 lm W-1
Max. EQE 26.8%


Device structure ITO/HAT-CN/TAPC/POSTF/POSTF:POT2T:15 mol% FIrpic/POSTF:PO-T2T:Ir(MDQ)2(acac)/PO-T2T/Liq/Al [2]
Colour White white
Max. Power Efficiency 60.7 lm W-1
Max. EQE 24.7%

 

Device structure ITO/HAT-CN/TAPC/ POSTF/POSTF:PO-T2T: 15% FIrpic (CRS)/PO-T2T/Liq/Al [2]
Colour Blue blue
Max. Power Efficiency 34.7 lm W-1
Max. EQE 20.1%

 

Device structure ITO/HAT-CN/TAPC/ POSTF/POSTF:PO-T2T: 15% FIrpic (CRS)/PO-T2T/Liq/Al [2]
Colour Blue blue
Max. Power Efficiency 57.4 lm W-1
Max. EQE 19.3%

 

Device structure ITO/HAT-CN/TAPC/ POSTF/POSTF:PO-T2T: 15% Ir(MDQ)2(acac) (CRS)/PO-T2T/Liq/Al [2]
Colour Red red
Max. Power Efficiency 46.0 lm W-1
Max. EQE 27.6%

 *For chemical structure information, please refer to the cited references.

Pricing

Grade Order Code Quantity Price
Sublimed (>99.0% purity) M2337A1 250 mg £289.00
Sublimed (>99.0% purity) M2337A1 500 mg £499.00
Sublimed (>99.0% purity) M2337A1 1 g £879.00

MSDS Documentation

POSTF MSDSPOSTF MSDS Sheet

Literature and Reviews

  1. Orthogonal Molecular Structure for Better Host Material in Blue Phosphorescence and Larger OLED White Lighting, L. Ding et al., Adv. Funct. Mater., 25 (4); 645-650 (2015); DOI: 10.1002/adfm.201403402.
  2. High-Quality White Organic Light-Emitting Diodes Composed of Binary Emitters with Color Rendering Index Exceeding 80 by Utilizing Color Remedy Strategy, X. Tang et al., Adv. Funct. Mater., 29 (11); 1807541 (2019); DOI: 10.1002/adfm.201807541.
  3. Theoretical Investigations of the Spiro-Annulated Triphenylamine/ N-Phenylcarbazole-Based Ambipolar Host Materials for OLEDs, D. Zhang, et al., ChemistrySelect, 2 (22), 6604-6611 (2017); DOI: 10.1002/slct.201701424.

To the best of our knowledge the information provided here is accurate. However, Ossila assume no liability for the accuracy of this page. The values provided are typical at the time of manufacture and may vary over time and from batch to batch. All products are for laboratory and research and development use only, and may not be used for any other purpose including health care, pharmaceuticals, cosmetics, food or commercial applications.

Return to the top