ITO Glass Substrates (Unpatterned)
These glass substrates are coated with a 100 nm layer of Indium Tin Oxide (ITO).

Useful for a variety of experimental techniques including microscopy (STM, conductive AFM), spectroscopy and electropolymerisation.
Specifications
Substrate sizes | 20mm x 15mm 25mm x 25mm 25mm x 75mm (Microscope Slide) |
Thickness | 1.1 mm |
Glass type | Polished soda lime, float glass |
Substrate coating | Fully oxidized ITO |
ITO thickness | 100 nm |
ITO quoted resistance | 20 Ω.□-1 |
ITO measured resistance* | 14 - 16 Ω.□-1 |
Glass roughness | 1 nm RMS (by AFM) |
ITO roughness | 1.8 nm RMS (by AFM) |
*Resistances measured using the Ossila Four-Point Probe System.
Currently, Ossila does not offer custom substrate sizes. We may offer additional sizes in the future based on demand. If you would like to make a suggestion, then please leave a request on our feedback page.
Characterisation


Transmittance of ITO Substrates

To the best of our knowledge the information provided here is accurate. However, Ossila assume no liability for the accuracy of this page. The values provided are typical at the time of manufacture and may vary over time and from batch to batch. All products are for laboratory and research and development use only, and may not be used for any other purpose including health care, pharmaceuticals, cosmetics, food or commercial applications.