TIPS Pentacene Data Sheet
6,13-bis(triisopropylsilylethinyl)pentacene commonly known as TIPS-pentacene

Generic Properties
| Appearance | Dark Blue Solid |
| Molecular Formula | C44H54Si2 |
| Molecular Weight | 639.07 |
| Solvents | Anisole, butylbenzene, chlorobenzene, chloroform, dichlorobenzene, tetrahydrofuran, toluene, xylene |
| Recommended solvent | Toluene |
| Recommended concentration | 10 mg/ml (drop cast / spin cast) |
Batch Specific Properties
| Batch Number | 49955 |
| Purity (HPLC) | >99.5% |
| Trace metal analysis (ICP OES) | Na, K, Sn, Mg, Ca, Zn, Al, Ba all < 5 PPM |
| DSC Endotherm melt onset | 255°C |
| DSC Exotherm onset | 260°C |
DSC trace
NMR trace
Crystallisation Images
Images below taken of thin films of TIPS-pentacene deposited by spin casting and drop casting from toluene (10 mg/ml) on SiO2 showing the strong crystallisation behaviour especially in slow dried films.