{"product_id":"toray-carbon-paper","title":"Toray Carbon Paper","description":"\u003ch2 id=\"product-oneliner\"\u003eRigid, non-woven carbon paper GDL substrate (TGP-H series)\u003c\/h2\u003e\n\u003cp class=\"text-center\"\u003eAvailable with or without PTFE wet-proofing treatment\u003cbr\u003e\u003c\/p\u003e\n\u003chr\u003e\n\u003cp class=\"text-center\"\u003e\u003ca href=\"#specification\"\u003eSpecifications\u003c\/a\u003e | \u003ca href=\"#gallery\"\u003eGallery\u003c\/a\u003e | \u003ca href=\"#pricing\"\u003ePricing and Options\u003c\/a\u003e | \u003ca href=\"#related-products\"\u003eRelated Products\u003c\/a\u003e | \u003ca href=\"#selection\"\u003eUntreated vs Wet-Proofed\u003c\/a\u003e | \u003ca href=\"#technical-support\"\u003eTechnical Support\u003c\/a\u003e\u003c\/p\u003e\n\u003chr\u003e\n\u003cp\u003eToray carbon paper is a non-woven, porous sheet of carbonized fibres, available in two thicknesses: 0.19 mm (TGP-H-060) and 0.28 mm (TGP-H-090). A well-established reference grade for gas diffusion layer research, Toray Carbon Paper combines low electrical resistance with open porosity, perfect for gas and liquid transport.\u003c\/p\u003e\n\u003cp\u003eIts fibrous structure (78% porosity) allows reactants and products to move through the sheet while the carbon network carries current across it. Making it a dependable substrate wherever your catalyst layer needs efficient mass transport.\u003c\/p\u003e\n\u003ch3\u003eToray Carbon Paper Applications\u003c\/h3\u003e\n\u003chr\u003e\n\u003cul\u003e\n\u003cli\u003eFuel cells and water electrolyzers\u003c\/li\u003e\n\u003cli\u003eBatteries and supercapacitors\u003c\/li\u003e\n\u003cli\u003eGas diffusion electrode (GDE flow cells)\u003c\/li\u003e\n\u003cli\u003eStandard Three-electrode Setups\u003c\/li\u003e\n\u003cli\u003eCO\u003csub\u003e2\u003c\/sub\u003e reduction reactors\u003c\/li\u003e\n\u003cli\u003eSensors\u003c\/li\u003e\n\u003c\/ul\u003e\n\u003cp\u003eToray paper is made by forming a carbon fibre web, binding it with a thermoset resin, and heat treating it at a high temperature. Resulting in a flat, rigid sheet with low in-plane resistance (5.6–5.8 mΩ·cm), flexural strength of 40 MPa, and a smooth surface (8 µm roughness). That rigidity gives consistent, predictable behaviour in a clamped cell. \n\u003c\/p\u003e\u003cp\u003e\u003cstrong\u003eImportant Note:\u003c\/strong\u003e Carbon paper is less compressible and more brittle than cloth-based substrates, so edges and corners require careful handling.\u003c\/p\u003e\n\u003cp\u003eToray Carbon Paper is available in two treatment options. Untreated (without PTFE wet-proofing and without a microporous layer), or treated (with 20% PTFE wet-proofing). This gives you the option of a clean starting point if you want to apply your own catalyst layer, coating, surface treatment, or if you plan to use the paper as a conductive and mechanical backing layer. For reference, adding PTFE makes the paper more hydrophobic and helps prevent flooding of the pores during operation, but higher PTFE loadings reduce conductivity.\u003c\/p\u003e\n\u003cp\u003e\u003cstrong\u003eNote:\u003c\/strong\u003e Porosity, compressibility, and handling behaviour differ between manufacturers and grades.\u003c\/p\u003e\n\u003cdiv class=\"row display-flex\"\u003e\n\u003cdiv class=\"col-xs-12 col-sm-4 col-md-3 text-center margin-top\"\u003e\n\u003cimg loading=\"lazy\" width=\"50\" height=\"50\" src=\"https:\/\/www.ossila.com\/cdn\/shop\/files\/highly-porous-icon.svg\"\u003e\n\u003cp class=\"blue-heading no-margin text-center\"\u003eHighly Porous\u003c\/p\u003e\n\u003cp class=\"text-center\"\u003e78% void volume, allowing gas and liquid transport through \u003c\/p\u003e\n\u003c\/div\u003e\n\u003cdiv class=\"col-xs-12 col-sm-4 col-md-3 text-center margin-top\"\u003e\n\u003cimg loading=\"lazy\" width=\"50\" height=\"50\" src=\"https:\/\/www.ossila.com\/cdn\/shop\/files\/conductive-icon.svg\"\u003e\n\u003cp class=\"blue-heading no-margin text-center\"\u003eElectrically Conductive\u003c\/p\u003e\n\u003cp class=\"text-center\"\u003eHigh conductivity = Efficient Current Collector\u003c\/p\u003e\n\u003c\/div\u003e\n\u003cdiv class=\"col-xs-12 col-sm-4 col-md-3 text-center margin-top\"\u003e\n\u003cimg loading=\"lazy\" width=\"50\" height=\"50\" src=\"https:\/\/www.ossila.com\/cdn\/shop\/files\/volume-level-icon.svg\"\u003e\n\u003cp class=\"blue-heading no-margin text-center\"\u003eHydrophobic (PTFE-treated only) \u003c\/p\u003e\n\u003cp class=\"text-center\"\u003ePrevents flooding of the porous structure during operation\u003c\/p\u003e\n\u003c\/div\u003e\n\u003cdiv class=\"col-xs-12 col-sm-4 col-md-3 text-center margin-top\"\u003e\n\u003cimg loading=\"lazy\" width=\"50\" height=\"50\" src=\"https:\/\/www.ossila.com\/cdn\/shop\/files\/chemically-inert-icon.svg\"\u003e\n\u003cp class=\"blue-heading no-margin text-center\"\u003eThermal and Chemical Stability\u003c\/p\u003e\n\u003cp class=\"text-center\"\u003eStable across a range operating temperatures and pH levels\u003c\/p\u003e\n\u003c\/div\u003e\n\u003c\/div\u003e\n\u003ch2 id=\"specification\"\u003eSpecifications\u003c\/h2\u003e\n\u003chr\u003e\n\u003ch3\u003eToray Carbon Paper\u003c\/h3\u003e\n\u003ctable style=\"width: 100%; height: 591.469px;\"\u003e\n\u003cthead\u003e\n\u003ctr style=\"height: 19.5938px;\"\u003e\n\u003cth width=\"38.2%\" style=\"width: 21.0835%; height: 19.5938px;\"\u003eProduct Code\u003c\/th\u003e\n\u003ctd style=\"width: 41.2502%; height: 19.5938px;\"\u003eC2061C20\u003c\/td\u003e\n\u003ctd style=\"width: 37.0807%; height: 19.5938px;\"\u003eC2061C30\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003c\/thead\u003e\n\u003ctbody\u003e\n\u003ctr\u003e\n\u003cth style=\"width: 21.0835%;\"\u003eManufacturer Code\u003c\/th\u003e\n\u003ctd style=\"width: 41.2502%;\"\u003eTGP-H-60\u003c\/td\u003e\n\u003ctd style=\"width: 37.0807%;\"\u003eTGP-H-90\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr style=\"height: 19.5938px;\"\u003e\n\u003cth width=\"38.2%\" style=\"width: 21.0835%; height: 19.5938px;\"\u003eThickness\u003c\/th\u003e\n\u003ctd style=\"width: 41.2502%; height: 19.5938px;\"\u003e0.19 mm\u003c\/td\u003e\n\u003ctd style=\"width: 37.0807%; height: 19.5938px;\"\u003e0.28 mm\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr style=\"height: 19.5938px;\"\u003e\n\u003cth width=\"38.2%\" style=\"width: 21.0835%; height: 19.5938px;\"\u003eWet Proofing\u003c\/th\u003e\n\u003ctd style=\"width: 41.2502%; height: 19.5938px;\"\u003eNo\u003c\/td\u003e\n\u003ctd style=\"width: 37.0807%; height: 19.5938px;\"\u003eNo\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr style=\"height: 19.5938px;\"\u003e\n\u003cth width=\"38.2%\" style=\"width: 21.0835%; height: 19.5938px;\"\u003eDimensions\u003c\/th\u003e\n\u003ctd style=\"width: 41.2502%; height: 19.5938px;\"\u003e20 cm × 20 cm\u003c\/td\u003e\n\u003ctd style=\"width: 37.0807%; height: 19.5938px;\"\u003e20 cm × 20 cm\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr style=\"height: 19.5938px;\"\u003e\n\u003cth width=\"38.2%\" style=\"width: 21.0835%; height: 19.5938px;\"\u003ePorosity\u003c\/th\u003e\n\u003ctd style=\"width: 41.2502%; height: 19.5938px;\"\u003e78%\u003c\/td\u003e\n\u003ctd style=\"width: 37.0807%; height: 19.5938px;\"\u003e78%\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr style=\"height: 23.25px;\"\u003e\n\u003cth width=\"38.2%\" style=\"width: 21.0835%; height: 23.25px;\"\u003eGas Permeability\u003c\/th\u003e\n\u003ctd style=\"width: 41.2502%; height: 23.25px;\"\u003e1900 ml·mm \/ [cm\u003csup\u003e2\u003c\/sup\u003e·hr·mmAq]\u003c\/td\u003e\n\u003ctd style=\"width: 37.0807%; height: 23.25px;\"\u003e1700 ml·mm \/ [cm\u003csup\u003e2\u003c\/sup\u003e·hr·mmAq]\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr style=\"height: 39.1875px;\"\u003e\n\u003cth width=\"38.2%\" style=\"width: 21.0835%; height: 39.1875px;\"\u003eResistance (in-plane)\u003c\/th\u003e\n\u003ctd style=\"width: 41.2502%; height: 39.1875px;\"\u003e5.8 mΩ·cm\u003c\/td\u003e\n\u003ctd style=\"width: 37.0807%; height: 39.1875px;\"\u003e5.6 mΩ·cm\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr style=\"height: 39.1875px;\"\u003e\n\u003cth width=\"38.2%\" style=\"width: 21.0835%; height: 39.1875px;\"\u003eResistance (through-plane)\u003c\/th\u003e\n\u003ctd style=\"width: 41.2502%; height: 39.1875px;\"\u003e80 mΩ·cm\u003c\/td\u003e\n\u003ctd style=\"width: 37.0807%; height: 39.1875px;\"\u003e80 mΩ·cm\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr style=\"height: 39.1875px;\"\u003e\n\u003cth width=\"38.2%\" style=\"width: 21.0835%; height: 39.1875px;\"\u003eFlexural Strength\u003c\/th\u003e\n\u003ctd style=\"width: 41.2502%; height: 39.1875px;\"\u003e40 MPa\u003c\/td\u003e\n\u003ctd style=\"width: 37.0807%; height: 39.1875px;\"\u003e40 MPa\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr style=\"height: 39.1875px;\"\u003e\n\u003cth width=\"38.2%\" style=\"width: 21.0835%; height: 39.1875px;\"\u003eSurface Roughness\u003c\/th\u003e\n\u003ctd style=\"width: 41.2502%; height: 39.1875px;\"\u003e8 µm\u003c\/td\u003e\n\u003ctd style=\"width: 37.0807%; height: 39.1875px;\"\u003e8 µm\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr style=\"height: 78.375px;\"\u003e\n\u003cth width=\"38.2%\" style=\"width: 21.0835%; height: 78.375px;\"\u003eThermal Conductivity: Through Plane (Room Temp)\u003c\/th\u003e\n\u003ctd style=\"width: 41.2502%; height: 78.375px;\"\u003e1.7 W \/m.K\u003c\/td\u003e\n\u003ctd style=\"width: 37.0807%; height: 78.375px;\"\u003e1.7 W \/m.K\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr style=\"height: 78.375px;\"\u003e\n\u003cth width=\"38.2%\" style=\"width: 21.0835%; height: 78.375px;\"\u003eThermal Conductivity: In-plane (Room Temp)\u003c\/th\u003e\n\u003ctd style=\"width: 41.2502%; height: 78.375px;\"\u003e21 W \/m.K\u003c\/td\u003e\n\u003ctd style=\"width: 37.0807%; height: 78.375px;\"\u003e21 W \/m.K\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr style=\"height: 58.7812px;\"\u003e\n\u003cth width=\"38.2%\" style=\"width: 21.0835%; height: 58.7812px;\"\u003eThermal Conductivity: In-plane (100°C)\u003c\/th\u003e\n\u003ctd style=\"width: 41.2502%; height: 58.7812px;\"\u003e23 W \/m.K\u003c\/td\u003e\n\u003ctd style=\"width: 37.0807%; height: 58.7812px;\"\u003e23 W \/m.K\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr style=\"height: 78.375px;\"\u003e\n\u003cth width=\"38.2%\" style=\"width: 21.0835%; height: 78.375px;\"\u003eIn-plane Coefficient of Thermal Expansion\u003c\/th\u003e\n\u003ctd style=\"width: 41.2502%; height: 78.375px;\"\u003e-0.8 × 10\u003csup\u003e-6\u003c\/sup\u003e\/°C\u003c\/td\u003e\n\u003ctd style=\"width: 37.0807%; height: 78.375px;\"\u003e-0.8 × 10\u003csup\u003e-6\u003c\/sup\u003e\/°C\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003c\/tbody\u003e\n\u003c\/table\u003e\n\u003ch2 id=\"gallery\"\u003eConductive Carbon Paper Gallery\u003c\/h2\u003e\n\u003chr\u003e\n\u003cdiv class=\"inline-block-container\"\u003e\n\u003cfigure class=\"double-float-left\"\u003e\u003cimg width=\"417.156\" src=\"https:\/\/www.ossila.com\/cdn\/shop\/files\/c2061m20-structure.jpg?v\u0026amp;width=417\" loading=\"lazy\" height=\"304\" class=\"fill\" alt=\"C2061M20 structure (TGP-H-60 with 20% PTFE wet proofing)\"\u003e\n\u003cfigcaption\u003eC2061M20 structure (TGP-H-60 with 20% PTFE wet proofing)\u003c\/figcaption\u003e\n\u003c\/figure\u003e\n\u003cfigure class=\"double-float-right\"\u003e\u003cimg width=\"417.156\" src=\"https:\/\/www.ossila.com\/cdn\/shop\/files\/c2061c20-structure.jpg?v\u0026amp;width=417\" loading=\"lazy\" height=\"304\" class=\"fill\" alt=\"C2061C20 structure (TGP-H-60 without wet proofing)\"\u003e\n\u003cfigcaption\u003eC2061C20 structure (TGP-H-60 without wet proofing)\u003c\/figcaption\u003e\n\u003c\/figure\u003e\n\u003c\/div\u003e\n\u003ch2 id=\"pricing\"\u003ePricing and Options\u003c\/h2\u003e\n\u003chr\u003e\n\u003ch3\u003eToray Carbon Paper Pricing\u003c\/h3\u003e\n\u003ctable\u003e\n\u003ctbody\u003e\n\u003ctr\u003e\n\u003cth width=\"38.2%\"\u003eProduct Code\u003c\/th\u003e\n\u003cth width=\"38.2%\"\u003eThickness\u003c\/th\u003e\n\u003cth width=\"38.2%\"\u003eWet Proofing\u003c\/th\u003e\n\u003cth width=\"38.2%\"\u003ePrice\u003c\/th\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eC2061C20\u003c\/td\u003e\n\u003ctd\u003e0.2 mm\u003c\/td\u003e\n\u003ctd\u003e0% (Hydrophilic)\u003c\/td\u003e\n\u003ctd\u003e£80\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eC2061M20\u003c\/td\u003e\n\u003ctd\u003e0.2 mm\u003c\/td\u003e\n\u003ctd\u003e20% (Hydrophobic)\u003c\/td\u003e\n\u003ctd\u003e£150\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003c\/tbody\u003e\n\u003c\/table\u003e\n\u003ch2\u003e\u003cbr\u003e\u003c\/h2\u003e\n\u003ch2 id=\"selection\"\u003eUntreated vs Wet-Proofed\u003c\/h2\u003e\n\u003chr\u003e\n\u003cdiv class=\"row pad-half-height\"\u003e\n\u003cdiv class=\"col-sm-12 col-md-6\"\u003e\n\u003ch3\u003eWithout PTFE (Untreated)\u003c\/h3\u003e\n\u003cul\u003e\n\u003cli\u003eCustom catalyst layer coating: gives full control over the catalyst–substrate interface, which suits early-stage electrode development and catalyst ink deposition.\u003c\/li\u003e\n\u003cli\u003eElectrode backing \/ current collector: a rigid, conductive support behind a catalyst-coated membrane or active layer, particularly in benchtop and H-cell configurations.\u003c\/li\u003e\n\u003cli\u003eSurface functionalisation: electrodeposition, spray coating, or drop-casting onto a bare surface avoids interference from an existing PTFE layer.\u003c\/li\u003e\n\u003cli\u003eOperando and spectroelectrochemical setups: an untreated sheet gives more uniform optical and electrical behaviour before modification, which helps when you need optical or spectroscopic access to the working electrode..\u003c\/li\u003e\n\u003c\/ul\u003e\n\u003c\/div\u003e\n\u003cdiv class=\"col-sm-12 col-md-6\"\u003e\n\u003ch3\u003eWith PTFE (Wet-Proofed)\u003c\/h3\u003e\n\u003cul\u003e\n\u003cli\u003eFuel cell and electrolyser gas diffusion layers: PTFE manages water balance in the pores, preventing flooding while keeping gas pathways open to the catalyst layer..\u003c\/li\u003e\n\u003cli\u003eGDE flow cells for CO₂ reduction: wet-proofing helps hold a stable gas\/liquid\/solid boundary at the catalyst layer, which supports consistent CO₂RR performance and limits electrolyte breakthrough.\u003c\/li\u003e\n\u003cli\u003eWater electrolysis benchmarking: as a gas-side diffusion layer or inert current collector in PEM\/AEM test cells, controlled hydrophobicity improves run-to-run reproducibility.\u003c\/li\u003e\n\u003c\/ul\u003e\n\u003c\/div\u003e\n\u003c\/div\u003e\n\u003cfigure\u003e\u003cimg alt=\"Treated Conductive Carbon Paper\" height=\"477\" loading=\"lazy\" src=\"https:\/\/www.ossila.com\/cdn\/shop\/files\/hydrophobic-carbon-paper.svg\" width=\"636\"\u003e\n\u003cfigcaption\u003eTreated and Untreated Conductive Carbon Paper\u003c\/figcaption\u003e\n\u003c\/figure\u003e\n\u003ch2 id=\"related-products\"\u003eRelated Products\u003c\/h2\u003e\n\u003chr\u003e\n\u003cdiv class=\"product-row\"\u003e\n\u003cdiv class=\"product-container text-center\"\u003e\u003ca href=\"https:\/\/www.ossila.com\/products\/porous-solid-electrolyte-reactor\"\u003e\u003cimg alt=\"Porous Solid Electrolyte Reactor\" class=\"product-image img-responsive\" height=\"190\" loading=\"lazy\" src=\"https:\/\/www.ossila.com\/cdn\/shop\/files\/porous-solid-electrolyte-reactor-product-photo.jpg?v=1784715301\u0026amp;width=190\" width=\"190\"\u003e\n\u003cp class=\"h4 word-wrap margin-bottom-small product-name\"\u003ePorous Solid Electrolyte Reactor\u003c\/p\u003e\n\u003c\/a\u003e\u003c\/div\u003e\n\u003cdiv class=\"product-container text-center\"\u003e\u003ca href=\"https:\/\/www.ossila.com\/products\/membrane-electrode-assembly-electrolyzer\"\u003e\u003cimg alt=\"Membrane Electrode Assembly Electrolyzer\" class=\"product-image img-responsive\" height=\"190\" loading=\"lazy\" src=\"https:\/\/www.ossila.com\/cdn\/shop\/files\/membrane-electrode-assembly-electrolyzer-product-photo.jpg?v=1781689564\u0026amp;width=190\" width=\"190\"\u003e\n\u003cp class=\"h4 word-wrap margin-bottom-small product-name\"\u003eMembrane Electrode Assembly Electrolyzer\u003c\/p\u003e\n\u003c\/a\u003e\u003c\/div\u003e\n\u003cdiv class=\"product-container text-center\"\u003e\u003ca href=\"https:\/\/www.ossila.com\/products\/advanced-gde-flow-cell\"\u003e\u003cimg alt=\"Advanced GDE Flow Cell\" class=\"product-image img-responsive\" height=\"190\" loading=\"lazy\" src=\"https:\/\/www.ossila.com\/cdn\/shop\/files\/advanced-gde-flow-cell-product-photo.jpg?v=1784624292\u0026amp;width=190\" width=\"190\"\u003e\n\u003cp class=\"h4 word-wrap margin-bottom-small product-name\"\u003eAdvanced GDE Flow Cell\u003c\/p\u003e\n\u003c\/a\u003e\u003c\/div\u003e\n\u003cdiv class=\"product-container text-center\"\u003e\u003ca href=\"https:\/\/www.ossila.com\/products\/in-situ-raman-electrochemical-cell\"\u003e\u003cimg alt=\"In-situ Raman Electrochemical Cell\" class=\"product-image img-responsive\" height=\"190\" loading=\"lazy\" src=\"https:\/\/www.ossila.com\/cdn\/shop\/files\/in-situ-raman-electrochemical-cell-c2035r1-product-photo.jpg?v=1718705939\u0026amp;width=190\" width=\"190\"\u003e\n\u003cp class=\"h4 word-wrap margin-bottom-small product-name\"\u003eIn-situ Raman Electrochemical Cell\u003c\/p\u003e\n\u003c\/a\u003e\u003c\/div\u003e\n\u003cdiv class=\"product-container text-center\"\u003e\u003ca href=\"https:\/\/www.ossila.com\/products\/gas-diffusion-raman-electrochemical-cell\"\u003e\u003cimg alt=\"Gas Diffusion In-situ Raman Electrochemical Cell\" class=\"product-image img-responsive\" height=\"190\" loading=\"lazy\" src=\"https:\/\/www.ossila.com\/cdn\/shop\/files\/gas-diffusion-in-situ-raman-electrochemical-cell-product-photo.jpg?v=1718705939\u0026amp;width=190\" width=\"190\"\u003e\n\u003cp class=\"h4 word-wrap margin-bottom-small product-name\"\u003eGas Diffusion In-situ Raman Electrochemical Cell\u003c\/p\u003e\n\u003c\/a\u003e\u003c\/div\u003e\n\u003c\/div\u003e\n\u003cdiv class=\"collection-container\"\u003e\n\u003cdiv class=\"collection-tile\"\u003e\u003ca href=\"\/collections\/spectroelectrochemical-cells\"\u003e\n\u003cdiv class=\"collection-button background-ossila-blue\"\u003e\n\u003cimg alt=\"Spectroelectrochemical Cells Collection\" height=\"109\" loading=\"lazy\" src=\"https:\/\/www.ossila.com\/cdn\/shop\/files\/spectroelectrochemical-collection-design.png?v\" width=\"150\"\u003e\n\u003cp\u003e\u003cstrong\u003eSpectro-\u003cbr\u003eelectrochemical Cells\u003c\/strong\u003e\u003c\/p\u003e\n\u003c\/div\u003e\n\u003c\/a\u003e\u003c\/div\u003e\n\u003cdiv class=\"collection-tile\"\u003e\u003ca href=\"\/collections\/mea-electrolyzer\"\u003e\n\u003cdiv class=\"collection-button background-light-blue\"\u003e\n\u003cimg width=\"150\" src=\"https:\/\/www.ossila.com\/cdn\/shop\/files\/membrane-electrode-assembly-collection-design.png?v=1715167619\" loading=\"lazy\" height=\"109\" alt=\"MEA Electrolyzers Collection\"\u003e\n\u003cp\u003e\u003cstrong\u003eMEA Electrolyzers\u003c\/strong\u003e\u003c\/p\u003e\n\u003c\/div\u003e\n\u003c\/a\u003e\u003c\/div\u003e\n\u003cdiv class=\"collection-tile\"\u003e\n\u003cdiv class=\"collection-button background-ossila-blue\"\u003e\n\u003ca href=\"\/collections\/flow-cells\"\u003e\u003cimg width=\"150\" src=\"https:\/\/www.ossila.com\/cdn\/shop\/files\/gde-flow-cell-collection-design.png?v=1715167618\" loading=\"lazy\" height=\"109\" alt=\"Flow Cells Collection\"\u003e\u003c\/a\u003e\n\u003cp\u003e\u003cstrong\u003eGDE Flow Cells\u003c\/strong\u003e\u003c\/p\u003e\n\u003c\/div\u003e\n\u003c\/div\u003e\n\u003c\/div\u003e","brand":"Ossila","offers":[{"title":"0%(Hydrophilic)","offer_id":52830289756376,"sku":"C2061C20","price":120.0,"currency_code":"USD","in_stock":true},{"title":"20%(Hydrophobic)","offer_id":52830289789144,"sku":"C2061M20","price":225.0,"currency_code":"USD","in_stock":true}],"thumbnail_url":"\/\/cdn.shopify.com\/s\/files\/1\/0823\/0287\/files\/toray-carbon-paper-product-photo.jpg?v=1788444191","url":"https:\/\/www.ossila.com\/products\/toray-carbon-paper","provider":"Ossila","version":"1.0","type":"link"}