Stir Bars (Halogenated Solvent Safe for Ink Preparation)

Order Code: C151

Price

(excluding Taxes)

£9.00


Oval PTFE coated stir bars for 4 ml vials. Stir bars that have been specifically designed to maximise stirring in our 4 ml amber vials. A virgin PTFE coating ensures maximum solvent compatibility. Designed to be disposable but also re-usable depending on usage and cleaning.

Diameter: 6 mm

Length: 10 mm

 

To the best of our knowledge the technical information provided here is accurate. However, Ossila assume no liability for the accuracy of this information. The values provided here are typical at the time of manufacture and may vary over time and from batch to batch.