ITO Glass Photovoltaic Substrates (8 Pixel)

Pre-patterned ITO Glass substrates for OPV/OLED testing. Use with our cathode deposition mask (E501) to create 8 individual pixels or (E502) to create a single large pixel.
Datasheet
Substrate size | 20 mm x 15 mm |
Thickness | 1.1 mm |
Glass type | Polished soda lime, float glass |
Substrate coating | Fully oxidized ITO |
ITO thickness | 100 nm |
ITO resistance | 20 Ω / square |
Glass roughness | < 1 nm RMS (By AFM) |
ITO roughness | 1.8 nm RMS (By AFM) |




To the best of our knowledge, the information provided here is accurate. However, Ossila assume no liability for the accuracy of this information. The values provided here are typical at the time of manufacture and may vary over time and from batch to batch.