PV and OLED Scale-Up Substrates (Modules)

Order Code: S251

Price

(excluding Taxes)

£525.00


A 25 X 75 mm ITO patterned glass substrate with modules for use in OPV and OLED research.

The Scale-Up and Mini-Module Substrate System is designed to enable affordable scale up. Alongside the Scale Up Substrate Evaporation Masks, the substrates allow for larger devices and investigation of large scale manufacture techniques. 


The Scale Up Modules OPV/OLED Patterned ITO Substrate

Datasheet

Size 25 mm x 75 mm
Thickness 1.1 mm
Glass type Polished soda lime, float glass
Substrate coating Fully oxidized ITO
ITO thickness 100 nm
ITO resistance 20 Ω/square
Glass roughness Less than 1 nm RMS (by AFM)
ITO roughness 1.8 nm RMS (by AFM)

Dimensions


Dimensionised Drawing of the Modules OPV/OLED Scale-up Substrate