PBT1, for highly efficient OPV devices
High purity and available online for priority dispatch
As a family member of polythiophenes, PBT1 (also known as PBDD4T), CAS number 1439937-09-3, has a backbone consisting of repeating benzodithiophene-4,8-dione and α-quaterthiophene units. π electrons can be delocalized effectively through the alternative electron push−pull effect, resulting a low band-gap polymer. Also, with four ethylhexyl branched side chains, the polymer is more soluble in most of organic solvents.
We also have PBDD4T-2F available which allows fluorine-fluorine interaction at the polymer back-bone structure for device film morphology control. Both PBDD4T and PBDD4T-2F are used for highly efficient OPV devices using fullerenes and non-fullerenes such as ITIC and P(NDI2OD-T2F) as acceptors.
Luminosyn™ PBT1
Luminosyn™ PBT1 is now available.
High purity and high molecular weight
PBDD4T is purified by Soxhlet extraction with methanol, hexane and chloroform under an argon atmosphere
Batch-specific GPC data
Have confidence in what you are ordering; batch-specific GPC data for your thesis or publications
Large quantity orders
Plan your experiments with confidence with polymers from the same batch
General Information
Full name | Poly[[5,7-bis(2-ethylhexyl)-4,8-dioxo-4H,8H-benzo[1,2-c:4,5-c']dithiophene-1,3-diyl][3,3'''-bis(2-ethylhexyl)[2,2':5',2'':5'',2'''-quaterthiophene]-5,5'''-diyl]] |
Synonyms | PBT1, BDD4T |
Chemical formula | (C58H74O2S6)n |
CAS number | 1439937-09-3 |
Solubility | Chloroform, chlorobenzene and dichlorobenzene (solution processing solvent chlorobenzene or dichlorobenzene) |
HOMO / LUMO | HOMO = -5.30 eV, Eg = 1.76 eV [1] |
Classification / Family | Polythiophenes, Organic n-type semiconducting materials, Organic photovoltaics, Polymer solar cells, Tandem solar cells, Electron-acceptor polymers, OFETs, Perovskite solar cells, All-polymer solar cells. |
Solubility | Soluble in chloroform, chlorobenzene, dichlorobenzene |
Chemical Structure
MSDS Documentation
Pricing
Batch | Quantity | Price |
M2049A1 | 100 mg | £420 |
M2049A1 | 250 mg | £800 |
M2049A1 | 500 mg | £1450 |
M2049A1 | 1 g | £2600 |
M2049A1 | 5 - 10 g* | Please enquire |
*for 5-10 grams order quantity, the lead time is 4-6 weeks.
Batch details
Batch | Mw | Mn | PDI | Stock Info |
M2049A1 | 112,851 | 49,310 | 2.29 | in stock |
Literature and Reviews
- A Fluorinated Polythiophene Derivative with Stabilized Backbone Conformation for Highly Efficient Fullerene and Non-Fullerene Polymer Solar Cells, S. Zhang et al., Macromolecules, 49 (8), 2993–3000 (2016); DOI: 10.1021/acs.macromol.6b00248.
- Molecular Design toward Efficient Polymer Solar Cells with High Polymer Content, D. Qian et al., J. Am. Chem. Soc., 2013, 135 (23), 8464–8467 (2013); DOI: 10.1021/ja402971d.
- Toward reliable and accurate evaluation of polymer solar cells based on low band gap polymers, L. Ye et al., J. Mater. Chem. C, 3, 564-569 (2015); DOI: 10.1039/C4TC02449D.