Ossila has sourced some of the most pure lead (II) chloride (PbCl2 ) available in order to provide you with confidence in materials used in your research.
Lead chloride is used as a precursor material in the fabrication of methyl ammonium lead iodide-chloride (MAPbI
3-x Cl
x ) perovskites. Using high purity lead chloride eliminates the effects that unknown sources of impurities can have on your experimental results. Ossila also offers premade inks using our high purity lead chloride for the fabrication of
MAPbI 3-x Cl x perovskites, these inks are based around
processing in air , or
processing in an inert atmosphere .
Please be aware that due to dangerous goods restrictions we are unable to ship lead chloride to some countries; please check whether your country is affected by contacting us for more information.
General Information
CAS number
7758-95-4
Chemical formula
PbCl 2
Synonyms
PbCl , Lead dichloride
Appearance
White/beige powder with chunks
Purity
99.999%
Molecular weight
278.10 g/mol
Density
5.85 g/mL at 25°C
Melting Point
501°C
Boiling Point
950°C
Solubility
Aliphatic hydrocarbons (slightly soluble)
Classification / Family
Perovskite precursor materials, Perovskite solar cells
Light-emitting diodes.