ITO Connection Substrates

Order Code: S191

Price

(excluding Taxes)

£425.00


Standard 20 x 15 mm float glass substrates with 20 nm synthetic quartz coating and connection strips of 100 nm of ITO.

A total of twelve connections are possible and encapsulation is available for the central area of 12.5 x 15 mm.

 

Datasheet

Size 20 mm x 15 mm
Thickness 1.1 mm
Glass type Polished soda lime, float glass
Substrate coating Fully oxidized ITO
ITO thickness 100 nm
ITO resistance 20 Ω/square
Glass roughness Less than 1 nm RMS (by AFM)
ITO roughness 1.8 nm RMS (by AFM)

 

ITO connection substrate schematic

 

AFM scan of ITO substrate
10 µm x 10 µm AFM scan with Z-scale of ±5 nm.

 

AFM of glass surface of ITO substrates
AFM of glass surface (1 µm x 1 µm x 3.5 nm). Courtesy of Richard T Grant.

 

Prepatterned ITO substrate absorption spectrum
Absorption of ITO substrates with and without PEDOT:PSS and epoxy/coverslip

 

Download data as Excel spreadsheet here.

 