Ossila have extended their range of ITO coated glass to include ITO coated microscope slides. These can be used for a wide variety of applications including biological imaging, spectroscopic studies of materials, and for the scale up processing of thin film devices.

 

Datasheet

Size 25 mm x 75 mm
Thickness 1.1 mm
Glass type Polished soda lime, float glass
Substrate coating Fully oxidised ITO
ITO thickness 100 nm
ITO resistance 20 Ω/square
Glass roughness 1 nm RMS (by AFM)
ITO roughness 1.8 nm RMS (by AFM)

 