Unpatterned ITO Coated Glass Substrates

Datasheet

Size 25 mm x 75 mm
Thickness 1.1 mm
Glass type Polished soda lime, float glass
Substrate coating Fully oxidized ITO
ITO thickness 100 nm
ITO resistance 20 Ω/square
Glass roughness 1 nm RMS (by AFM)
ITO roughness 1.8 nm RMS (by AFM)