Video: How to Make Solution Processed OFETs Quickly and Easily

This video describes how to make solution based OFETs quickly and simply using our pre-patterned ITO substrates to act as the source-drain contacts along with a polymeric insulator (PMMA) and gate (PEDOT:PSS).

Make your own OFETs

Since very little equipment is required, these OFETs are easy to make in your own lab and also great for teaching and training purposes: contact our OFET team for more information, buy the pre-patterend OFET substrates featured in the video or view our full range of OFET, TFT and sensor products.