This video demonstrates how to load the long channel OFET stack used to thermally evaporate (vacuum deposit) source-drain contacts. The video shows the below steps:

  1. Loading the mask onto the lower support.

  2. Loading the substrate support holder

  3. Loading a substrate

  4. Adding the magnetic sheet

  5. Screwing the lid on