Tungsten Disulfide (WS2) Crystal
Tungsten Disulfide Crystal, high purity 2D semiconducting TMDCs material
For applications in light-emitting devices, solar cells, and photodetectors
Like other TMDC family members, tungsten disulfide (WS2) has a two-dimensional structure. It consists of a layer of hexagonally-arranged tungsten atoms positioned between two layers of hexagonally-arranged sulphur atoms.
Individual layers are held together by Van der Waals forces. This makes it possible for single to few-layer ultra-thin films to be prepared from bulk crystals using mechanical exfoliation techniques. The primitive unit cell of WS2 consists of one tungsten atom and two sulphur atoms, arranged in a trigonal prismatic configuration.
With a photoluminescence (PL) quantum yield that is almost two orders of magnitude higher at room temperature than MoS2, WS2 is one of the most popular 2D semiconducting TMDCs materials, and is widely explored for applications in light-emitting devices, solar cells, and photodetectors.
Structure of Tungsten Disulfide Crystal

Platinum FET Test Chips for 2D Materials

- Affordable
- World-Wide Shipping
- Dual Channel Electrodes
Buy Online £180.00
Applications of Tungsten Disulfide Crystal
In the form of single or few-layer thin films, exfoliated WS2 nanosheets find applications ranging from light emitters, field effect transistors (FETs) and photovoltaics. Like many other TMDCs, they are actively used in condensed matter physics and photonics research.
Synthesis
Tungsten disulfide WS2 is manufactured using chemical vapour transport (CVT) crystallisation, with crystals having a purity in excess of 99.999%.
Usage
Tungsten disulfide WS2 can be used to prepare monolayer and few-layer WS2 by mechanical or liquid exfoliation.
Viscoelastic transfer of 2D material using PDMS
Literature and Reviews
- Controlled Synthesis and Transfer of Large-Area WS2 Sheets: From Single Layer to Few Layers, A. Elı´as et al., ACS Nano, 7 (6), 5235–5242 (2013); DOI: 10.1021/nn400971k.
- Extraordinary Room-Temperature Photoluminescence in Triangular WS2 Monolayers, H. R. Gutiérrez et al., Nano Lett., 13 (8), 3447–3454 (2013); DOI: 10.1021/nl3026357.
- Controlled Growth of High-Quality Monolayer WS2 Layers on Sapphire and Imaging Its Grain Boundary, Y. Zhang et al., ACS Nano, 7 (10), 8963–8971 (2013); DOI: 10.1021/nn403454e.
- Photosensor Device Based on Few-Layered WS2 Films, N. Perea-López et al., Adv. Funct. Mater., 23, 5511–5517 (2013); DOI: 10.1002/adfm.201300760.
- Direct Chemical Vapor Deposition Growth of WS2 Atomic Layers on Hexagonal Boron Nitride, M. Okada et al., ACS Nano, 8 (8), 8273–8277 (2014); DOI: 10.1021/nn503093k.
Technical Data
CAS Number | 12138-09-9 |
Chemical Formula | WS2 |
Molecular Weight | 247.97 g/mol |
Bandgap | 1.4 - 2.01 eV [1] |
Preparation | Synthetic - Chemical Vapour Transport (CVT) |
Structure | Hexagonal |
Electronic Properties | 2D semiconductor |
Melting {oint | 1250 °C (lit.) |
Colour | Black |
Synonyms | Tungsten sulphide, Tungsten sulfide, Tungsten(IV) sulfide |
Classification / Family | Transition metal dichalcogenides (TMDCs), 2D semiconductor materials, Nano-electronics, Nano-photonics, Materials science |
Product Details
Form | Purity |
Crystal | ≥99.999% |
MSDS Document
Pricing Table
Product Code | Form | Size* | Quantity (EA) | Price |
M2110A10 | Crystal | Small (≥10 mm2) | 1 | £480.00 |
M2110A25 | Crystal | Medium (≥25 mm2) | 1 | £760.00 |
M2110A00 | Crystal | Large** (≥100 mm2) | 1 | £1600.00 |
*typical representative size, areas/dimensions may vary
**item with a lead time of 2 - 3 weeks, please contact for more information
To the best of our knowledge the information provided here is accurate. However, Ossila assume no liability for the accuracy of this page. The values provided are typical at the time of manufacture and may vary over time and from batch to batch. All products are for laboratory and research and development use only, and may not be used for any other purpose including health care, pharmaceuticals, cosmetics, food or commercial applications.