General Information

CAS number 566939-58-0  
Chemical formula C14H17Br2NO2S
Molecular weight 423.16 g/mol
Synonyms TPD-C8, 2,5-Dibromo-N-n-octyl-3,4-thiophenedicarboximide
Classification / Family Thiophene, Heterocyclic five-membered ring, Organic semiconducting materials, Semiconductor Synthesis, Low band gap polymers, OFETs, OLED, Organic Photovoltaics, Polymer Solar Cells

Chemical Structure

TPD-C8, 1,3-Dibromo-5-octyl-4H-thieno[3,4-c]pyrrole-4,6(5H)-dione, 566939-58-0
Chemical structure of 1,3-Dibromo-5-octyl-4H-thieno[3,4-c]pyrrole-4,6(5H)-dione

Product Details

Purity > 99%
Melting point 105-109 °C
Appearance Orange powder/crystals

MSDS Documentation

TPD-C8 MSDSTPD-C8 MSDS Sheet

Literature and Reviews

  1. Alkoxyl Side Chain Substituted Thieno[3,4-c]pyrrole-4,6-dione To Enhance Photovoltaic Performance with Low Steric Hindrance and High Dipole Moment, Macromolecules, 49 (16), pp 5788–5795 (2016); DOI: 10.1021/acs.macromol.6b00927.
  2. Synthesis of new D-A polymers containing disilanobithiophene donor and application to bulk heterojunction polymer solar cells, M. Nakashima et al, Polymer J., 47, 733–738 (2015); doi:10.1038/pj.2015.61.
  3. Low band gap dithienogermolodithiophene copolymers with tunable acceptors and side-chains for organic solar cells, H. Zhong et al., J. Mater. Chem. A, 1, 14973-14981 (2013); DOI: 10.1039/C3TA13778C.

To the best of our knowledge the information provided here is accurate. However, Ossila assume no liability for the accuracy of this page. The values provided are typical at the time of manufacture and may vary over time and from batch to batch. All products are for laboratory and research and development use only, and may not be used for any other purpose including health care, pharmaceuticals, cosmetics, food or commercial applications.

Return to the top