1,4,8,11-tetramethyl-6,13-triethylsilylethynyl pentacene also known as TMTES-Pentacene. It is a soluble derivative of Pentacene [1], achieving mobilities of up to 4.34 cm2/Vs. TMTES-Pentacene is an ideal small-molecule semiconductor for both device fabrication and investigating the charge transport of solution-processed crystal semiconductor [4]. Mobilities of 3.5 cm2/Vs have been measured when spin coated using CYTOP© as the gate dielectric [2], and mobilities of up to 4.34 cm2/Vs have been achieved when used with high-permittivity polymer binders [3].
General Information
Full name | 1,4,8,11-tetramethyl-6,13-triethylsilylethynyl pentacene |
---|---|
Synonyms | TMTES-pentacene |
CAS number | n/a |
Molecular formula | C42H50Si2 |
Molecular weight | 611.017 g/mol |
Appearance | Black crystalline solid |
Solvents | Anisole, butylbenzene, chlorobenzene, chloroform, dichlorobenzene, tetrahydrofuran, toluene, xylene |
Recommended solvent | Toluene |
Recommended concentration | 10 mg/ml (drop cast / spin cast) |

Characterisation

References
(Please note that Ossila has no formal connection to any other authors or institutions in these references):
[1] High performance, acene-based organic thin film transistors. Gonzalo R Llorente et al., Chem. Commun., p3059-3061 (2009)
[2] Charge-transport physics of high-mobility molecular semiconductors. H Sirringhaus et al., Status Solidi B., V 9, 1655-1676 (2012)
[3] High Performance Organic Transistors Using Small Molecule Semiconductors and High Permittivity Semiconducting Polymers. Keri L McCall et al., Advanced Functional Materials, V 17, Issue 17, p3421-3434 (2007)
[4] Hall-Effect Measurements Probing the Degree of Charge-Carrier Delocalization in Solution-Processed Crystalline Molecular Semiconductors. Jui-Fen Chang et al., PhysRe Lett, V 107, 066601 (2011)
To the best of our knowledge the information provided here is accurate. However, Ossila assume no liability for the accuracy of this page. The values provided are typical at the time of manufacture and may vary over time and from batch to batch. All products are for laboratory and research and development use only, and may not be used for any other purpose including health care, pharmaceuticals, cosmetics, food or commercial applications.