2,4,6-tris(biphenyl-3-yl)-1,3,5-triazine (T2T) is a family member of triazine. It has one electron-withdrawing triazine core and three electron-rich biphenyl groups. It has been widely used as a host material for phosphorescent OLEDs and electron transport layer material (ETL) for TADF-OLEDs.
Due to its electron-deficient nature, T2T and its derivatives are also used as acceptor materials to form exciplexes in blue-emission TADF devices.
*Sublimation is a technique used to obtain ultra pure-grade chemicals. For more details about sublimation, please refer to the Sublimed Materials for OLED devices page.
Chemical Structure
Chemical structure of 2,4,6-tris(biphenyl-3-yl)-1,3,5-triazine (T2T), CAS 1201800-83-0.
Operational stability enhancement in organic light-emitting diodes with ultrathin Liq interlayers, D. Tsang et al., Sci. Rep., 6:22463 (2016); DOI: 10.1038/srep22463.
1,3,5-Triazine derivatives as new electron transport–type host materials forhighly efficient green phosphorescent OLEDs, H-F. Chen et al., J. Mater. Chem., 19, 8112–8118 (2009); DOI: 10.1039/b913423a.
Thermally activated delayed-fluorescence organic light-emitting diodes based on exciplex emitter with high efficiency and low roll-off, T. Lin et al., Org. Electronics, 38, 69-73 (2016); DIO: 10.1016/j.orgel.2016.08.001.
High-efficiency organic light-emitting diodes with fluorescent emitters, H. Nakanotani et al., Nat. Commun., 5:4016 (2014); DOI: 10.1038/ncomms5016.
Dual enhancement of electroluminescence efficiency and operational stability by rapid upconversion of triplet excitons in OLEDs, T. Furukawa1 et al., Sci. Rep., 5:8429 (2015) DOI: 10.1038/srep08429.
To the best of our knowledge the information provided here is accurate. However, Ossila assume no liability for the accuracy of this page. The values provided are typical at the time of manufacture and may vary over time and from batch to batch. All products are for laboratory and research and development use only, and may not be used for any other purpose including health care, pharmaceuticals, cosmetics, food or commercial applications.